Structure, mechanical properties and degradation behavior of electrospun PEEU fiber meshes and films

  • The capability of a degradable implant to provide mechanical support depends on its degradation behavior. Hydrolytic degradation was studied for a polyesteretherurethane (PEEU70), which consists of poly(p-dioxanone) (PPDO) and poly(epsilon-caprolactone) (PCL) segments with a weight ratio of 70:30 linked by diurethane junction units. PEEU70 samples prepared in the form of meshes with average fiber diameters of 1.5 mu m (mesh1.5) and 1.2 mu m (mesh1.2), and films were sterilized and incubated in PBS at 37 degrees C with 5 vol% CO2 supply for 1 to 6 weeks. Degradation features, such as cracks or wrinkles, became apparent from week 4 for all samples. Mass loss was found to be 11 wt%, 6 wt%, and 4 wt% for mesh1.2, mesh1.5, and films at week 6. The elongation at break decreased to under 20% in two weeks for mesh1.2. In case of the other two samples, this level of degradation was achieved after 4 weeks. The weight average molecular weight of both PEEU70 mesh and film samples decreased to below 30 kg/mol when elongation at break dropped belowThe capability of a degradable implant to provide mechanical support depends on its degradation behavior. Hydrolytic degradation was studied for a polyesteretherurethane (PEEU70), which consists of poly(p-dioxanone) (PPDO) and poly(epsilon-caprolactone) (PCL) segments with a weight ratio of 70:30 linked by diurethane junction units. PEEU70 samples prepared in the form of meshes with average fiber diameters of 1.5 mu m (mesh1.5) and 1.2 mu m (mesh1.2), and films were sterilized and incubated in PBS at 37 degrees C with 5 vol% CO2 supply for 1 to 6 weeks. Degradation features, such as cracks or wrinkles, became apparent from week 4 for all samples. Mass loss was found to be 11 wt%, 6 wt%, and 4 wt% for mesh1.2, mesh1.5, and films at week 6. The elongation at break decreased to under 20% in two weeks for mesh1.2. In case of the other two samples, this level of degradation was achieved after 4 weeks. The weight average molecular weight of both PEEU70 mesh and film samples decreased to below 30 kg/mol when elongation at break dropped below 20%. The time period of sustained mechanical stability of PEEU70-based meshes depends on the fiber diameter and molecular weight.show moreshow less

Export metadata

Additional Services

Search Google Scholar Statistics
Metadaten
Author details:Wing Tai TungGND, Xianlei SunGND, Weiwei WangGND, Xun XuORCiD, Nan MaORCiD, Andreas LendleinORCiDGND
DOI:https://doi.org/10.1557/s43580-020-00001-0
ISSN:2059-8521
Title of parent work (English):MRS advances : a journal of the Materials Research Society (MRS)
Publisher:Springer Nature Switzerland AG
Place of publishing:Cham
Publication type:Article
Language:English
Date of first publication:2021/03/11
Publication year:2021
Release date:2024/06/10
Volume:6
Issue:10
Number of pages:7
First page:276
Last Page:282
Funding institution:Projekt DEAL
Organizational units:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Chemie
Mathematisch-Naturwissenschaftliche Fakultät / Institut für Biochemie und Biologie
DDC classification:5 Naturwissenschaften und Mathematik / 54 Chemie / 540 Chemie und zugeordnete Wissenschaften
5 Naturwissenschaften und Mathematik / 57 Biowissenschaften; Biologie / 570 Biowissenschaften; Biologie
Peer review:Referiert
Publishing method:Open Access / Hybrid Open-Access
License (German):License LogoCC-BY - Namensnennung 4.0 International
Accept ✔
This website uses technically necessary session cookies. By continuing to use the website, you agree to this. You can find our privacy policy here.