The residual stress in as-built laser powder bed fusion IN718 alloy as a consequence of the scanning strategy induced microstructure

  • The effect of two types of scanning strategies on the grain structure and build-up of Residual Stress (RS) has been investigated in an as-built IN718 alloy produced by Laser Powder Bed Fusion (LPBF). The RS state has been investigated by X-ray diffraction techniques. The microstructural characterization was performed principally by Electron Backscatter Diffraction (EBSD), where the application of a post-measurement refinement technique enables small misorientations (< 2 degrees) to be resolved. Kernel average misorientation (KAM) distributions indicate that preferably oriented columnar grains contain higher levels of misorientation, when compared to elongated grains with lower texture. The KAM distributions combined with X-ray diffraction stress maps infer that the increased misorientation is induced via plastic deformation driven by the thermal stresses, acting to self-relieve stress. The possibility of obtaining lower RS states in the build direction as a consequence of the influence of the microstructure should be considered whenThe effect of two types of scanning strategies on the grain structure and build-up of Residual Stress (RS) has been investigated in an as-built IN718 alloy produced by Laser Powder Bed Fusion (LPBF). The RS state has been investigated by X-ray diffraction techniques. The microstructural characterization was performed principally by Electron Backscatter Diffraction (EBSD), where the application of a post-measurement refinement technique enables small misorientations (< 2 degrees) to be resolved. Kernel average misorientation (KAM) distributions indicate that preferably oriented columnar grains contain higher levels of misorientation, when compared to elongated grains with lower texture. The KAM distributions combined with X-ray diffraction stress maps infer that the increased misorientation is induced via plastic deformation driven by the thermal stresses, acting to self-relieve stress. The possibility of obtaining lower RS states in the build direction as a consequence of the influence of the microstructure should be considered when envisaging scanning strategies aimed at the mitigation of RS.show moreshow less

Export metadata

Additional Services

Search Google Scholar Statistics
Metadaten
Author details:Itziar Serrano-MunozORCiD, Tatiana MishurovaORCiDGND, Tobias ThiedeORCiDGND, Maximilian SprengelORCiD, Arne KrommORCiDGND, Naresh Nadammal, Gert Nolze, Romeo Saliwan-Neumann, Alexander EvansORCiD, Giovanni BrunoORCiDGND
DOI:https://doi.org/10.1038/s41598-020-71112-9
ISSN:2045-2322
Pubmed ID:https://pubmed.ncbi.nlm.nih.gov/32887914
Title of parent work (English):Scientific reports
Publisher:Macmillan Publishers Limited, part of Springer Nature
Place of publishing:London
Publication type:Article
Language:English
Date of first publication:2020/09/04
Publication year:2020
Release date:2023/03/24
Tag:EBSD; components; deposition; diffraction; distortion; heat-treatment; mechanical properties; melting slm; superalloys; texture
Volume:10
Issue:1
Article number:14645
Number of pages:15
Funding institution:Projekt DEAL
Organizational units:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Physik und Astronomie
DDC classification:5 Naturwissenschaften und Mathematik / 50 Naturwissenschaften / 500 Naturwissenschaften und Mathematik
6 Technik, Medizin, angewandte Wissenschaften / 60 Technik / 600 Technik, Technologie
Peer review:Referiert
Publishing method:Open Access / Gold Open-Access
License (German):License LogoCC-BY - Namensnennung 4.0 International
Accept ✔
This website uses technically necessary session cookies. By continuing to use the website, you agree to this. You can find our privacy policy here.