Isoprene and beta-myrcene were polymerized by anionic polymerization in bulk and in the 'green' ether solvents cyclopentyl methyl ether and 2-methyltetrahydrofuran and, for comparison, in cyclohexane and tetrahydrofuran. The polydienes produced in bulk and in cyclohexane contained high amounts of 1,4 units (>90%) whereas those produced in ether solvents were rich in 1,2 and 3,4 units (36%-86%). Comparison of the microstructures and glass transition temperatures of the polydienes obtained in the various solvents suggests that conventionally used solvents can be substituted by environmentally more friendly alternatives.
We report a 1,2,3-triazol fluoroionophore for detecting Na+ that shows in vitro enhancement in the Na+-induced fluorescence intensity and decay time. The Na+-selective molecule 1 was incorporated into a hydrogel as a part of a fiber optical sensor. This sensor allows the direct determination of Na+ in the range of 1–10 mM by measuring reversible fluorescence decay time changes.