Refine
Year of publication
Document Type
- Article (2399)
- Doctoral Thesis (669)
- Postprint (170)
- Monograph/Edited Volume (60)
- Review (31)
- Other (30)
- Habilitation Thesis (15)
- Conference Proceeding (14)
- Preprint (8)
- Part of a Book (1)
- Master's Thesis (1)
Is part of the Bibliography
- yes (3398) (remove)
Keywords
- nanoparticles (29)
- self-assembly (24)
- Nanopartikel (21)
- DNA origami (20)
- biomaterials (19)
- ionic liquids (17)
- polymer (17)
- block copolymers (16)
- fluorescence (16)
- Polymer (15)
Institute
- Institut für Chemie (3398) (remove)
In recent years, due to its great promise in boosting the energy density of lithium batteries for future energy storage, research on the Li metal anode, as an alternative to the graphite anode in Li-ion batteries, has gained significant momentum. However, the practical use of Li metal anodes has been plagued by unstable Li (re)deposition and poor cyclability. Although tremendous efforts have been devoted to the stabilization of Li metal anodes, the mechanisms of electrochemical (re-)deposition/dissolution of Li and solid-electrolyte-interphase (SEI) formation remain elusive. This article highlights the recent mechanistic understandings and observations of Li deposition/dissolution and SEI formation achieved from advanced characterization techniques and simulation methods, and discusses major limitations and open questions in these processes. In particular, the authors provide their perspectives on advanced and emerging/potential methods for obtaining new insights into these questions. In addition, they give an outlook into cutting-edge interdisciplinary research topics for Li metal anodes. It pushes beyond the current knowledge and is expected to accelerate development toward a more in-depth and comprehensive understanding, in order to guide future research on Li metal anodes toward practical application.
Die vorliegende Arbeit thematisiert die Synthese und die Polymerisation von Monomeren auf der Basis nachwachsender Rohstoffe wie zum Beispiel in Gewürzen und ätherischen Ölen enthaltenen kommerziell verfügbaren Phenylpropanoiden (Eugenol, Isoeugenol, Zimtalkohol, Anethol und Estragol) und des Terpenoids Myrtenol sowie ausgehend von der Rinde einer Birke (Betula pendula) und der Korkeiche (Quercus suber). Ausgewählte Phenylpropanoide (Eugenol, Isoeugenol und Zimtalkohol) und das Terpenoid Myrtenol wurden zunächst in den jeweiligen Laurylester überführt und anschließend das olefinische Strukturelement epoxidiert, wobei 4 neue (2-Methoxy-4-(oxiran-2-ylmethyl)phenyldodecanoat, 2-Methoxy-4-(3-methyl-oxiran-2-yl)phenyldodecanoat, (3-Phenyloxiran-2-yl)methyldodecanoat, (7,7-Dimethyl-3-oxatricyclo[4.1.1.02,4]octan-2-yl)methyldodecanoat) und 2 bereits bekannte monofunktionelle Epoxide (2-(4-Methoxybenzyl)oxiran und 2-(4-Methoxyphenyl)-3-methyloxiran) erhalten wurden, die mittels 1H-NMR-, 13C-NMR- und FT-IR-Spektroskopie sowie mit DSC untersucht wurden. Die Photo-DSC Untersuchung der Epoxidmonomere in einer kationischen Photopolymerisation bei 40 °C ergab die maximale Polymerisationsgeschwindigkeit (Rpmax: 0,005 s-1 bis 0,038 s-1) sowie die Zeit (tmax: 13 s bis 26 s) bis zum Erreichen des Rpmax-Wertes und führte zu flüssigen Oligomeren, deren zahlenmittlerer Polymerisationsgrad mit 3 bis 6 mittels GPC bestimmt wurde. Die Umsetzung von 2-Methoxy-4-(oxiran-2-ylmethyl)phenyldodecanoat mit Methacrylsäure ergab ein Isomerengemisch (2-Methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat und 2-Methoxy-4-(2-(methacryl-oyloxy)-3-hydroxypropyl)phenyldodecanoat), das mittels Photo-DSC in einer freien radikalischen Photopolymerisation untersucht wurde (Rpmax: 0,105 s-1 und tmax: 5 s), die zu festen in Chloroform unlöslichen Polymeren führte.
Aus Korkpulver und gemahlener Birkenrinde wurden selektiv 2 kristalline
ω-Hydroxyfettsäuren (9,10-Epoxy-18-hydroxyoctadecansäure und 22-Hydroxydocosansäure) isoliert. Die kationische Photopolymerisation der 9,10-Epoxy-18-hydroxyoctadecansäure ergab einen nahezu farblosen transparenten und bei Raumtemperatur elastischen Film, welcher ein Anwendungspotential für Oberflächenbeschichtungen hat. Aus der Reaktion von 9,10-Epoxy-18-hydroxyoctadecansäure mit Methacrylsäure wurde ein bei Raumtemperatur flüssiges Gemisch aus zwei Konstitutionsisomeren (9,18-Dihydroxy-10-(methacryloyl-oxy)octadecansäure und 9-(Methacryloyloxy)-10,18-dihydroxyoctadecansäure) erhalten
(Tg: -60 °C). Die radikalische Photopolymerisation dieser Konstitutionsisomere wurde ebenfalls mittels Photo-DSC untersucht (Rpmax: 0,098 s-1 und tmax: 3,8 s). Die Reaktion von 22-Hydroxydocosansäure mit Methacryloylchlorid ergab die kristalline 22-(Methacryloyl-oxy)docosansäure, welche ebenfalls in einer radikalischen Photopolymerisation mittels Photo-DSC untersucht wurde (Rpmax: 0,023 s-1 und tmax: 9,6 s).
Die mittels AIBN in Dimethylsulfoxid initiierte Homopolymerisation der
22-(Methacryloyloxy)docosansäure und der Isomerengemische bestehend aus 2-Methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat und 2-Methoxy-4-(2-(methacryl-oyloxy)-3-hydroxypropyl)phenyldodecanoat sowie aus 9,18-Dihydroxy-10-(methacryloy-loxy)octadecansäure und 9-(Methacryloyloxy)-10,18-dihydroxyoctadecansäure ergab feste lösliche Polymere, die mittels 1H-NMR- und FT-IR-Spektroskopie, GPC (Poly(2-methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat / 2-methoxy-4-(2-(methacryloyl-oxy)-3-hydroxypropyl)phenyldodecanoat): Pn = 94) und DSC (Poly(2-methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat / 2-methoxy-4-(2-(methacryloyloxy)-3-hydroxypropyl)phenyldodecanoat): Tg: 52 °C; Poly(9,18-dihydroxy-10-(methacryloyloxy)-octadecansäure / 9-(methacryloyloxy)-10,18-dihydroxyoctadecansäure): Tg: 10 °C; Poly(22-(methacryloyloxy)docosansäure): Tm: 74,1 °C, wobei der Schmelzpunkt mit dem des Photopolymers (Tm = 76,8 °C) vergleichbar ist) charakterisiert wurden.
Das bereits bekannte Monomer 4-(4-Methacryloyloxyphenyl)butan-2-on wurde ausgehend von 4-(4-Hydroxyphenyl)butan-2-on hergestellt, welches aus Birkenrinde gewonnen werden kann, und unter identischen Bedingungen für einen Vergleich mit den neuen Monomeren polymerisiert. Die freie radikalische Polymerisation führte zu Poly(4-(4-methacryloyloxy-phenyl)butan-2-on) (Pn: 214 und Tg: 83 °C). Neben der Homopolymerisation wurde eine statistische Copolymerisation des Isomerengemisches 2-Methoxy-4-(2-hydroxy-3-(methacryl-oyloxy)propyl)phenyldodecanoat / 2-Methoxy-4-(2-(methacryloyl-oxy)-3-hydroxypropyl)-phenyldodecanoat mit 4-(4-Methacryloyloxyphenyl)butan-2-on untersucht, wobei ein äquimolarer Einsatz der Ausgangsmonomere zu einem Anstieg der Ausbeute, der Molmassenverteilung und der Dispersität des Copolymers (Tg: 44 °C) führte. Die unter Verwendung von Diethylcarbonat als „grünes“ Lösungsmittel mittels AIBN initiierten freien radikalischen Homopolymerisationen von 4-(4-Methacryloyloxyphenyl)butan-2-on und von Laurylmethacrylat ergaben vergleichbare Polymerisationsgrade der Homopolymere (Pn: 150), welche jedoch aufgrund ihrer Strukturunterschiede deutlich unterschiedliche Glasübergangstemperaturen hatten (Poly(4-(4-methacryloyloxyphenyl)butan-2-on): Tg: 70 °C, Poly(laurylmethacrylat) Tg: -49 °C. Eine statistische Copolymerisation äquimolarer Stoffmengen der beiden Monomere in Diethylcarbonat führte bei einer Polymerisationszeit von 60 Minuten zu einem leicht bevorzugten Einbau des 4-(4-Methacryloyloxyphenyl)butan-2-on in das Copolymer (Tg: 17 °C). Copolymerisationsdiagramme für die freien radikalischen Copolymerisationen von 4-(4-Methacryloyloxyphenyl)butan-2-on mit n-Butylmethacrylat beziehungsweise 2-(Dimethylamino)ethylmethacrylat (t: 20 min bis 60 min; Molenbrüche (X) für 4-(4-Methacryloyloxyphenyl)butan-2-on: 0,2; 0,4; 0,6 und 0,8) zeigten ein nahezu ideales azeotropes Copolymerisationsverhalten, obwohl ein leicht bevorzugter Einbau von
4-(4-Methacryloyloxyphenyl)butan-2-on in das jeweilige Copolymer beobachtet wurde. Dabei korreliert ein Anstieg der Ausbeute und der Glasübergangstemperatur der erhaltenen Copolymere mit einem zunehmenden Gehalt an 4-(4-Methacryloyloxyphenyl)butan-2-on im Reaktionsgemisch. Die unter Einsatz der modifizierten Gibbs-DiMarzio-Gleichung berechneten Glasübergangstemperaturen der Copolymere stimmten mit den gemessenen Werten gut überein. Das ist eine gute Ausgangsbasis für die Bestimmung der Glasübergangstemperatur eines Copolymers mit einer beliebigen Zusammensetzung.
Following excited-state chemical shifts in molecular ultrafast x-ray photoelectron spectroscopy
(2022)
Imaging the charge flow in photoexcited molecules would provide key information on photophysical and photochemical processes. Here the authors demonstrate tracking in real time after photoexcitation the change in charge density at a specific site of 2-thiouracil using time-resolved X-ray photoelectron spectroscopy. The conversion of photon energy into other energetic forms in molecules is accompanied by charge moving on ultrafast timescales. We directly observe the charge motion at a specific site in an electronically excited molecule using time-resolved x-ray photoelectron spectroscopy (TR-XPS). We extend the concept of static chemical shift from conventional XPS by the excited-state chemical shift (ESCS), which is connected to the charge in the framework of a potential model. This allows us to invert TR-XPS spectra to the dynamic charge at a specific atom. We demonstrate the power of TR-XPS by using sulphur 2p-core-electron-emission probing to study the UV-excited dynamics of 2-thiouracil. The method allows us to discover that a major part of the population relaxes to the molecular ground state within 220-250 fs. In addition, a 250-fs oscillation, visible in the kinetic energy of the TR-XPS, reveals a coherent exchange of population among electronic states.
Self-assembly of plasmonic nanoantenna-waveguide structures for subdiffractional chiral sensing
(2021)
Spin-momentum locking is a peculiar effect in the near-field of guided optical or plasmonic modes. It can be utilized to map the spinning or handedness of electromagnetic fields onto the propagation direction. This motivates a method to probe the circular dichroism of an illuminated chiral object. In this work, we demonstrate local, subdiffraction limited chiral coupling of light and propagating surface plasmon polaritons in a self-assembled system of a gold nanoantenna and a silver nanowire. A thin silica shell around the nanowire provides precise distance control and also serves as a host for fluorescent molecules, which indicate the direction of plasmon propagation. We characterize our nanoantenna-nanowire systems comprehensively through correlated electron microscopy, energy-dispersive X-ray spectroscopy, dark-field, and fluorescence imaging. Three-dimensional numerical simulations support the experimental findings. Besides our measurement of far-field polarization, we estimate sensing capabilities and derive not only a sensitivity of 1 mdeg for the ellipticity of the light field, but also find 10(3) deg cm(2)/dmol for the circular dichroism of an analyte locally introduced in the hot spot of the antenna-wire system. Thorough modeling of a prototypical design predicts on-chip sensing of chiral analytes. This introduces our system as an ultracompact sensor for chiral response far below the diffraction limit.
Herein, the concept of constructing binder- and carbon additive-free organosulfur cathode was proved based on thiol-containing conducting polymer poly(4-(thiophene-3-yl) benzenethiol) (PTBT). The PTBT featured the polythiophene-structure main chain as a highly conducting framework and the benzenethiol side chain to copolymerize with sulfur and form a crosslinked organosulfur polymer (namely S/PTBT). Meanwhile, it could be in-situ deposited on the current collector by electro-polymerization, making it a binder-free and free-standing cathode for Li-S batteries. The S/PTBT cathode exhibited a reversible capacity of around 870 mAh g(-1) at 0.1 C and improved cycling performance compared to the physically mixed cathode (namely S&PTBT). This multifunction cathode eliminated the influence of the additives (carbon/binder), making it suitable to be applied as a model electrode for operando analysis. Operando X-ray imaging revealed the remarkable effect in the suppression of polysulfides shuttle via introducing covalent bonds, paving the way for the study of the intrinsic mechanisms in Li-S batteries.
In vitro thrombogenicity test systems require co-cultivation of endothelial cells and platelets under blood flow-like conditions. Here, a commercially available perfusion system is explored using plasma-treated cyclic olefin copolymer (COC) as a substrate for the endothelial cell layer. COC was characterized prior to endothelialization and co-cultivation with platelets under static or flow conditions. COC exhibits a low roughness and a moderate hydrophilicity. Flow promoted endothelial cell growth and prevented platelet adherence. These findings show the suitability of COC as substrate and the importance of blood flow-like conditions for the assessment of the thrombogenic risk of drugs or cardiovascular implant materials.
Recent advances in organic solar cell performance have been mainly driven forward by combining high-performance p-type donor-acceptor copolymers (e.g.PM6) and non-fullerene small molecule acceptors (e.g.Y6) as bulk-heterojunction layers. A general observation in such devices is that the device performance, e.g., the open-circuit voltage, is strongly dependent on the processing solvent. While the morphology is a typically named key parameter, the energetics of donor-acceptor blends are equally important, but less straightforward to access in the active multicomponent layer. Here, we propose to use spectral onsets during electrochemical cycling in a systematic spectroelectrochemical study of blend films to access the redox behavior and the frontier orbital energy levels of the individual compounds. Our study reveals that the highest occupied molecular orbital offset (Delta E-HOMO) in PM6:Y6 blends is similar to 0.3 eV, which is comparable to the binding energy of Y6 excitons and therefore implies a nearly zero driving force for the dissociation of Y6 excitons. Switching the PM6 orientation in the blend films from face-on to edge-on in bulk has only a minor influence on the positions of the energy levels, but shows significant differences in the open circuit voltage of the device. We explain this phenomenon by the different interfacial molecular orientations, which are known to affect the non-radiative decay rate of the charge-transfer state. We compare our results to ultraviolet photoelectron spectroscopy data, which shows distinct differences in the HOMO offsets in the PM6:Y6 blend compared to neat films. This highlights the necessity to measure the energy levels of the individual compounds in device-relevant blend films.
Structure, mechanical properties and degradation behavior of electrospun PEEU fiber meshes and films
(2021)
The capability of a degradable implant to provide mechanical support depends on its degradation behavior. Hydrolytic degradation was studied for a polyesteretherurethane (PEEU70), which consists of poly(p-dioxanone) (PPDO) and poly(epsilon-caprolactone) (PCL) segments with a weight ratio of 70:30 linked by diurethane junction units. PEEU70 samples prepared in the form of meshes with average fiber diameters of 1.5 mu m (mesh1.5) and 1.2 mu m (mesh1.2), and films were sterilized and incubated in PBS at 37 degrees C with 5 vol% CO2 supply for 1 to 6 weeks. Degradation features, such as cracks or wrinkles, became apparent from week 4 for all samples. Mass loss was found to be 11 wt%, 6 wt%, and 4 wt% for mesh1.2, mesh1.5, and films at week 6. The elongation at break decreased to under 20% in two weeks for mesh1.2. In case of the other two samples, this level of degradation was achieved after 4 weeks. The weight average molecular weight of both PEEU70 mesh and film samples decreased to below 30 kg/mol when elongation at break dropped below 20%. The time period of sustained mechanical stability of PEEU70-based meshes depends on the fiber diameter and molecular weight.
Plasmon-driven dehalogenation of brominated purines has been recently explored as a model system to understand fundamental aspects of plasmon-assisted chemical reactions. Here, it is shown that divalent Ca2+ ions strongly bridge the adsorption of bromoadenine (Br-Ade) to Ag surfaces.
Such ion-mediated binding increases the molecule's adsorption energy leading to an overlap of the metal energy states and the molecular states, enabling the chemical interface damping (CID) of the plasmon modes of the Ag nanostructures (i.e., direct electron transfer from the metal to Br-Ade).
Consequently, the conversion of Br-Ade to adenine almost doubles following the addition of Ca2+.
These experimental results, supported by theoretical calculations of the local density of states of the Ag/Br-Ade complex, indicate a change of the charge transfer pathway driving the dehalogenation reaction, from Landau damping (in the lack of Ca2+ ions) to CID (after the addition of Ca2+).
The results show that the surface dynamics of chemical species (including water molecules) play an essential role in charge transfer at plasmonic interfaces and cannot be ignored. It is envisioned that these results will help in designing more efficient nanoreactors, harnessing the full potential of plasmon-assisted chemistry.
Informatische Bildung spielt eine immer zentralere Rolle in der Bildung einer Gesellschaft des 21. Jahrhunderts. Für den Chemieunterricht ergeben sich daraus zwei Aspekte: Einerseits können Konzepte der informatischen Bildung dabei helfen, chemie- und naturwissenschaftsspezifische Denk- und Arbeitsweisen zu fördern. Andererseits kann der Chemieunterricht einen Beitrag für die informatische Bildung leisten. Dieser Artikel geht auf beide Aspekte ein und versucht die gegenseitigen Vorteile der informatischen Bildung und der naturwissenschaftlichen Bildung im Chemieunterricht darzustellen.