Isoprene and beta-myrcene were polymerized by anionic polymerization in bulk and in the 'green' ether solvents cyclopentyl methyl ether and 2-methyltetrahydrofuran and, for comparison, in cyclohexane and tetrahydrofuran. The polydienes produced in bulk and in cyclohexane contained high amounts of 1,4 units (>90%) whereas those produced in ether solvents were rich in 1,2 and 3,4 units (36%-86%). Comparison of the microstructures and glass transition temperatures of the polydienes obtained in the various solvents suggests that conventionally used solvents can be substituted by environmentally more friendly alternatives.
Epoxidized 1,4-polymyrcene
(2020)
1,4-Polymyrcene was synthesized by anionic polymerization and epoxidized using meta-chloroperbenzoic acid. Samples with different degrees of epoxidation (25%, 49%, 74%, and 98%) were prepared and examined according to their chemical and thermal properties. Epoxidation was found to increase the glass transition temperature (T-g = 14 degrees C for the 98% epoxidized 1,4-polymyrcene) as well as the shelf live (>10 months). The trisubstituted epoxide groups were remarkably stable against nucleophiles under basic conditions but cross-linked or hydrolyzed in the presence of an acid. Also, highly epoxidized 1,4-polymyrcene readily cross-linked upon annealing at 260 degrees C to produce an epoxy resin.