Simulation of volumetric swelling of degradable poly[(rac-lactide)-co-glycolide] based polyesterurethanes containing different urethane-linkers

  • Aim: The hydrolytic degradation behavior of degradable aliphatic polyester-based polymers is strongly influenced by the uptake or transport of water into the polymer matrix and also the hydrolysis rate of ester bonds. Methods: We examined the volumetric swelling behavior of poly[(rac-lactide)-co-glycolide] (PLGA) and PLGA-based polyurethanes (PLGA-PU) with water contents of 0 wt%, 2 wt% and 7 wt% water at 310 K using a molecular modeling approach. Polymer systems with a number average molecular weight of M-n = 10,126 g.mol(-1) were constructed from PLGA with a lactide content of 67 mol%, whereby PLGA-PU systems were composed of five PLGA segments with M-n = 2052 g.mol(-1), which were connected via urethane linkers originated from 2,2,4-trimethyl hexamethylene-1,6-diisocyanate (TMDI), hexamethyl-1,6-diisocyanate (HDI), or L-lysine-1,6-diisocyanate (LDI). Results: The calculated densities of the dry PLGA-PU systems were found to be lower than for pure PLGA. The obtained volumetric swelling of the PLGA-PU was depending on the type ofAim: The hydrolytic degradation behavior of degradable aliphatic polyester-based polymers is strongly influenced by the uptake or transport of water into the polymer matrix and also the hydrolysis rate of ester bonds. Methods: We examined the volumetric swelling behavior of poly[(rac-lactide)-co-glycolide] (PLGA) and PLGA-based polyurethanes (PLGA-PU) with water contents of 0 wt%, 2 wt% and 7 wt% water at 310 K using a molecular modeling approach. Polymer systems with a number average molecular weight of M-n = 10,126 g.mol(-1) were constructed from PLGA with a lactide content of 67 mol%, whereby PLGA-PU systems were composed of five PLGA segments with M-n = 2052 g.mol(-1), which were connected via urethane linkers originated from 2,2,4-trimethyl hexamethylene-1,6-diisocyanate (TMDI), hexamethyl-1,6-diisocyanate (HDI), or L-lysine-1,6-diisocyanate (LDI). Results: The calculated densities of the dry PLGA-PU systems were found to be lower than for pure PLGA. The obtained volumetric swelling of the PLGA-PU was depending on the type of urethane linker, whereby all swollen PLGA-PUs contained larger free volume distribution compared to pure PLGA. The mean square displacement curves for dry PLGA and PLGA-PUs showed that urethane linker units reduce the mobility of the polymer chains, while an increase in backbone atoms mobility was found, when water was added to these systems. Consequently, an increased water uptake of PLGA-PU matrices combined with a higher mobility of the chain segments should result in an accelerated hydrolytic chain scission rate in comparison to PLGA. Conclusions: It can be anticipated that the incorporation of urethane linkers might be a helpful tool to adjust the degradation behavior of polyesters.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Suche bei Google Scholar Statistik - Anzahl der Zugriffe auf das Dokument
Metadaten
Verfasserangaben:Ehsan Ghobadi, Matthias HeuchelORCiDGND, Karl KratzORCiD, Andreas LendleinORCiDGND
DOI:https://doi.org/10.5301/JABFM.2012.10432
ISSN:2280-8000
Titel des übergeordneten Werks (Englisch):Journal of applied biomaterials & functional materials
Verlag:Wichtig
Verlagsort:Milano
Publikationstyp:Wissenschaftlicher Artikel
Sprache:Englisch
Jahr der Erstveröffentlichung:2012
Erscheinungsjahr:2012
Datum der Freischaltung:26.03.2017
Freies Schlagwort / Tag:Hydrolytic degradation; Molecular dynamics simulation; Polyesterurethane
Band:10
Ausgabe:3
Seitenanzahl:9
Erste Seite:293
Letzte Seite:301
Organisationseinheiten:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Chemie
Peer Review:Referiert
Verstanden ✔
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.