Structural and photoluminescence characterization of mesoporous silicon-phosphates

  • Two different types of mesoporous silicon-phosphate supports using different surfactants (a mixture of (CH3)(3)C13H27NBr with an organophosphorus coupling molecule (HO-PO(i-C3H7)(2)) and with a co-surfactant ((C2H5)(3)(C6H5)PCl), respectively) were synthesized. Trivalent europium (Eu) ions were immobilized via ion-exchange on these supports. The resulting materials were characterized using nitrogen adsorption isotherms at -196 degrees C, thermogravimetric analysis, SEM, TEM, FT-IR, PXRD, CP/MAS. (HSi)-H-1-Si-29 and P-31 NMR, DR-UV-vis as well as steady- state and time-resolved photoluminescence spectroscopy. The results evidenced that the co-polymerization of silicon and phosphorous yielded a unique morphology in these materials. Following calcination at 450 and 900 degrees C europium- exchanged silicon-phosphates with great surface area (BET=600-705 m(2) g(-1)) and 3.4 nm sized mesopores were obtained. The differences among the optical properties of the non-calcined europium materials such as the emission lifetimes, local environmentTwo different types of mesoporous silicon-phosphate supports using different surfactants (a mixture of (CH3)(3)C13H27NBr with an organophosphorus coupling molecule (HO-PO(i-C3H7)(2)) and with a co-surfactant ((C2H5)(3)(C6H5)PCl), respectively) were synthesized. Trivalent europium (Eu) ions were immobilized via ion-exchange on these supports. The resulting materials were characterized using nitrogen adsorption isotherms at -196 degrees C, thermogravimetric analysis, SEM, TEM, FT-IR, PXRD, CP/MAS. (HSi)-H-1-Si-29 and P-31 NMR, DR-UV-vis as well as steady- state and time-resolved photoluminescence spectroscopy. The results evidenced that the co-polymerization of silicon and phosphorous yielded a unique morphology in these materials. Following calcination at 450 and 900 degrees C europium- exchanged silicon-phosphates with great surface area (BET=600-705 m(2) g(-1)) and 3.4 nm sized mesopores were obtained. The differences among the optical properties of the non-calcined europium materials such as the emission lifetimes, local environment at the europium sites or the relative contribution of the upper excited levels to the total photoluminescence were assigned to the surfactants used in the synthesis. Calcination of the silicon-phosphates at higher temperatures than 450 degrees C did not induce major changes in the structural properties: in contrast, photoluminescence properties of europium were markedly improved in terms of intensity and average lifetime.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Suche bei Google Scholar Statistik - Anzahl der Zugriffe auf das Dokument
Metadaten
Verfasserangaben:Carmen Tiseanu, Vasile Parvulescu, Victoria Parvulescu, Elena Cotoi, Andre Gessner, Michael Uwe KumkeORCiDGND, Simion Simon, Florin Vasiliu
URL:http://www.sciencedirect.com/science/journal/10106030
DOI:https://doi.org/10.1016/j.jphotochem.2010.07.015
ISSN:1010-6030
Publikationstyp:Wissenschaftlicher Artikel
Sprache:Englisch
Jahr der Erstveröffentlichung:2010
Erscheinungsjahr:2010
Datum der Freischaltung:25.03.2017
Quelle:Journal of photochemistry and photobiology : A chemistry. - ISSN 1010-6030. - 215 (2010), 1, S. 17 - 24
Organisationseinheiten:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Chemie
Peer Review:Referiert
Verstanden ✔
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.