pH-sensitivity and conformation change of the n-terminal methacrylated peptide VK20

  • N-terminal methacrylation of peptide MAXI, which is capable of conformational changes variation of the pH, results in a peptide, named VK20. Increasing the reactivity of this terminal group enables further coupling reactions or chemical modifications of the peptidc. However, this end group functionalization may influence the ability of confonnational changes of VK20; as well as its properties. In this paper; the influence of pH on the transition between random coil and beta-sheet conformation of VK20; including the transition kinetics, were investigated. At pH values of 9 and higher, the kinetics beta-sheet formation increased tor VK(2 0, compared to MAXI. The self-assembly into beta-sheets recognized by the formation of a physically crosslinked gel was furthermore indicated by a significant increase of G. An increase in pH (from 9 to 9.5) led to a faster gelation of the peptide VK20. Simultaneously, G was increased from 460 +/- 70 Pa (at pH 9) to 1520 +/- 180 Pa (at pH 9.5). At the nanoscale, the gel showed a highly interconnectedN-terminal methacrylation of peptide MAXI, which is capable of conformational changes variation of the pH, results in a peptide, named VK20. Increasing the reactivity of this terminal group enables further coupling reactions or chemical modifications of the peptidc. However, this end group functionalization may influence the ability of confonnational changes of VK20; as well as its properties. In this paper; the influence of pH on the transition between random coil and beta-sheet conformation of VK20; including the transition kinetics, were investigated. At pH values of 9 and higher, the kinetics beta-sheet formation increased tor VK(2 0, compared to MAXI. The self-assembly into beta-sheets recognized by the formation of a physically crosslinked gel was furthermore indicated by a significant increase of G. An increase in pH (from 9 to 9.5) led to a faster gelation of the peptide VK20. Simultaneously, G was increased from 460 +/- 70 Pa (at pH 9) to 1520 +/- 180 Pa (at pH 9.5). At the nanoscale, the gel showed a highly interconnected fibrillar/network structure with uniform fibril widths of approximately 3.4 +/- 0.5 nm (N=30). The recovery of the peptide conformation back to random coil resulted in the dissolution of the gel; whereby the kinetics of the recovery depended on the pH. Conclusively, the ability of MAXI to undergo confommtional changes was not affected by N-terminal methacrylation whereas the kinetics of pH-sensitive beta-sheet formations has been increased.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Suche bei Google Scholar Statistik - Anzahl der Zugriffe auf das Dokument
Metadaten
Verfasserangaben:Zewang YouGND, Marc BehlORCiDGND, Candy LöwenbergGND, Andreas LendleinORCiDGND
DOI:https://doi.org/10.1557/adv.2017.491
ISSN:2059-8521
Titel des übergeordneten Werks (Englisch):MRS advances : a journal of the Materials Research Society (MRS)
Verlag:Cambridge University Press
Verlagsort:Cambridge
Publikationstyp:Wissenschaftlicher Artikel
Sprache:Englisch
Datum der Erstveröffentlichung:17.07.2017
Erscheinungsjahr:2017
Datum der Freischaltung:12.09.2022
Band:2
Seitenanzahl:9
Erste Seite:2571
Letzte Seite:2579
Organisationseinheiten:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Chemie
DDC-Klassifikation:5 Naturwissenschaften und Mathematik / 54 Chemie / 540 Chemie und zugeordnete Wissenschaften
Peer Review:Referiert