@article{AdelsbergerGrilloKulkarnietal.2013, author = {Adelsberger, Joseph and Grillo, Isabelle and Kulkarni, Amit and Sharp, Melissa and Bivigou Koumba, Achille Mayelle and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Kinetics of aggregation in micellar solutions of thermoresponsive triblock copolymers - influence of concentration, start and target temperatures}, series = {Soft matter}, volume = {9}, journal = {Soft matter}, number = {5}, publisher = {Royal Society of Chemistry}, address = {Cambridge}, issn = {1744-683X}, doi = {10.1039/c2sm27152d}, pages = {1685 -- 1699}, year = {2013}, abstract = {In aqueous solution, symmetric triblock copolymers with a thermoresponsive middle block and hydrophobic end blocks form flower-like core-shell micelles which collapse and aggregate upon heating through the cloud point (CP). The collapse of the micellar shell and the intermicellar aggregation are followed in situ and in real-time using time-resolved small-angle neutron scattering (SANS), while heating micellar solutions of a poly((styrene-d(8))-b-(N-isopropyl acrylamide)-b-(styrene-d(8))) triblock copolymer in D2O rapidly through their CP. The influence of polymer concentration as well as of the start and target temperatures is addressed. In all cases, the micellar collapse is very fast. The collapsed micelles immediately form small clusters which contain voids. They densify which slows down or even stops their growth. For low concentrations and target temperatures just above the CP, i.e. shallow temperature jumps, the subsequent growth of the clusters is described by diffusion-limited aggregation. In contrast, for higher concentrations and/or higher target temperatures, i.e. deep temperature jumps, intermicellar bridges dominate the growth. Eventually, in all cases, the clusters coagulate which results in macroscopic phase separation. For shallow temperature jumps, the cluster surfaces stay rough; whereas for deep temperature jumps, a concentration gradient develops at late stages. These results are important for the development of conditions for thermal switching in applications, e.g. for the use of thermoresponsive micellar systems for transport and delivery purposes.}, language = {en} } @article{MiasnikovaLaschewskyDePaolietal.2012, author = {Miasnikova, Anna and Laschewsky, Andr{\´e} and De Paoli, Gabriele and Papadakis, Christine M. and M{\"u}ller-Buschbaum, Peter and Funari, Sergio S.}, title = {Thermoresponsive Hydrogels from Symmetrical Triblock Copolymers Poly(styrene-block-(methoxy diethylene glycol acrylate)-block-styrene)}, series = {Langmuir}, volume = {28}, journal = {Langmuir}, number = {9}, publisher = {American Chemical Society}, address = {Washington}, issn = {0743-7463}, doi = {10.1021/la204665q}, pages = {4479 -- 4490}, year = {2012}, abstract = {A series of symmetrical, thermo-responsive triblock copolymers was prepared by reversible addition fragmentation chain transfer (RAFT) polymerization, and studied in aqueous solution with respect to their ability to form hydrogels. Triblock copolymers were composed of two identical, permanently hydrophobic outer blocks, made of low molar mass polystyrene, and of a hydrophilic inner block of variable length, consisting of poly(methoxy diethylene glycol acrylate) PMDEGA. The polymers exhibited a LCST-type phase transition in the range of 20-40 degrees C, which markedly depended on molar mass and concentration. Accordingly, the triblock copolymers behaved as amphiphiles at low temperatures, but became water-insoluble at high temperatures. The temperature dependent self-assembly of the amphiphilic block copolymers in aqueous solution was studied by turbidimetry and rheology at concentrations up to 30 wt \%, to elucidate the impact of the inner thermoresponsive block on the gel properties. Additionally, small-angle X-ray scattering (SAXS) was performed to access the structural changes in the gel with temperature. For all polymers a gel phase was obtained at low temperatures, which underwent a gel-sol transition at intermediate temperatures, well below the cloud point where phase separation occurred. With increasing length of the PMDEGA inner block, the gel-sol transition shifts to markedly lower concentrations, as well as to higher transition temperatures. For the longest PMDEGA block studied (DPn about 450), gels had already formed at 3.5 wt \% at low temperatures. The gel-sol transition of the hydrogels and the LCST-type phase transition of the hydrophilic inner block were found to be independent of each other.}, language = {en} } @article{ZhongAdelsbergerNiedermeieretal.2013, author = {Zhong, Qi and Adelsberger, Joseph and Niedermeier, M. A. and Golosova, Anastasi and Bivigou Koumba, Achille Mayelle and Laschewsky, Andr{\´e} and Funari, S. S. and Papadakis, Christine M. and M{\"u}ller-Buschbaum, Peter}, title = {The influence of selective solvents on the transition behavior of poly(styrene-b-monomethoxydiethylenglycol-acrylate-b-styrene) thick films}, series = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, volume = {291}, journal = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, number = {6}, publisher = {Springer}, address = {New York}, issn = {0303-402X}, doi = {10.1007/s00396-012-2879-4}, pages = {1439 -- 1451}, year = {2013}, abstract = {Thick poly(styrene-b-monomethoxydiethylenglycol-acrylate-b-styrene) [P(S-b-MDEGA-b-S)] films (thickness 5 mu m) are prepared from different solvents on flexible substrates by solution casting and investigated with small-angle X-ray scattering. As the solvents are either PS- or PMDEGA-selective, micelles with different core-shell micellar structures are formed. In PMDEGA-selective solvents, the PS block is the core and PMDEGA is the shell, whereas in PS-selective solvents, the order is reversed. After exposing the films to liquid D2O, the micellar structure inside the films prepared from PMDEGA-selective solvents remains unchanged and only the PMDEGA (shell part) swells. On the contrary, in the films prepared from PS-selective solvents, the micelles revert the core and the shell. This reversal causes more entanglements of the PMDEGA chains between the micelles. Moreover, the thermal collapse transition of the PMDEGA block in liquid D2O is significantly broadened. Irrespective of the solvent used for film preparation, the swollen PMDEGA shell does not show a prominent shrinkage when passing the phase transition, and the transition process occurs via compaction. The collapsed micelles have a tendency to densely pack above the transition temperature.}, language = {en} } @article{AdelsbergerKulkarniJainetal.2010, author = {Adelsberger, Joseph and Kulkarni, Amit and Jain, Abhinav and Wang, Weinan and Bivigou Koumba, Achille Mayelle and Busch, Peter and Pipich, Vitaliy and Holderer, Olaf and Hellweg, Thomas and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Thermoresponsive PS-b-PNIPAM-b-PS micelles : aggregation behavior, segmental dynamics, and thermal response}, issn = {0024-9297}, doi = {10.1021/Ma902714p}, year = {2010}, abstract = {We have studied I lie thermal behavior of amphiphilic, symmetric triblock copolymers having short, deuterated polystyrene (PS) end blocks and a large poly(N-isopropylacrylarnicle) (PNIPAM) middle block exhibiting a lower critical solution temperature (LCST) in aqueous solution. A wide range of concentrations (0.1-300 mg/mL) is investigated using it number of analytical methods such as fluorescence correlation spectroscopy (FCS), turbidimetry, dynamic light scattering (DLS), small-angle neutron scattering (SANS), and neutron spin-echo spectroscopy (NSE). The critical micelle concentration is determined using FCS to be 1 mu M or less. The collapse of the micelles at the LCST is investigated using turbidimetry and DLS and shows a weak dependence on the degree of polymerization of the PNIPAM block. SANS with contrast matching allows its to reveal the core-shell Structure of the micelles as well as their correlation as a function of temperature. The segmental dynamics of the PNIPAM shell are studied as a function of temperature and arc found to be faster in the collapsed state than in the swollen state. The mode detected has a linear dispersion in q(2) and is found to be faster in the collapsed state as compared to the swollen state. We attribute this result to the averaging over mobile and immobilized segments.}, language = {en} } @article{BivigouKoumbaGoernitzLaschewskyetal.2010, author = {Bivigou Koumba, Achille Mayelle and Goernitz, Eckhard and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Thermoresponsive amphiphilic symmetrical triblock copolymers with a hydrophilic middle block made of poly(N- isopropylacrylamide) : synthesis, self-organization, and hydrogel formation}, issn = {0303-402X}, doi = {10.1007/s00396-009-2179-9}, year = {2010}, abstract = {Several series of symmetrical triblock copolymers were synthesized by the reversible addition fragmentation chain transfer method. They consist of a long block of poly(N-isopropylacrylamide) as hydrophilic, thermoresponsive middle block, which is end-capped by two small strongly hydrophobic blocks made from five different vinyl polymers. The association of the amphiphilic polymers was studied in dilute and concentrated aqueous solution. The polymer micelles found at low concentrations form hydrogels at high concentrations, typically above 30-35 wt.\%. Hydrogel formation and the thermosensitive rheological behavior were studied exemplarily for copolymers with hydrophobic blocks of polystyrene, poly(2-ethylhexyl acrylate), and poly(n-octadecyl acrylate). All systems exhibited a cloud point around 30 A degrees C. Heating beyond the cloud point initially favors hydrogel formation but continued heating results in macroscopic phase separation. The rheological behavior suggests that the copolymers associate into flower-like micelles, with only a small share of polymers that bridge the micelles and act as physical cross-linkers, even at high concentrations.}, language = {en} } @article{BivigouKoumbaKristenLaschewskyetal.2009, author = {Bivigou Koumba, Achille Mayelle and Kristen, Juliane and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Synthesis of symmetrical triblock copolymers of styrene and N-isopropylacrylamide using bifunctional bis(trithiocarbonate)s as RAFT agents}, issn = {1022-1352}, doi = {10.1002/macp.200800575}, year = {2009}, abstract = {Six new bifunctional bis(trithiocarbonate)s were explored as RAFT agents for synthesizing amphiphilic triblock copolymers ABA and BAB, with hydrophilic "A" blocks made from N-isopropylacrylamide and hydrophobic "B" blocks made from styrene. Whereas the extension of poly(N-isopropylacrylamide) by styrene was not effective, polystyrene macroRAFT agents provided the block copolymers efficiently. End group analysis by H-1 NMR spectroscopy supported molar mass analysis and revealed an unexpected side reaction for certain bis(trithiocarbonate)s, namely a fragmentation to simple trithiocarbonates while extruding ethylene-trithiocarbonate. The amphiphilic block copolymers with short polystyrene blocks are directly soluble in water and self-organize into thermo-responsive micellar aggregates.}, language = {en} } @article{KyriakosAravopoulouAugsbachetal.2014, author = {Kyriakos, Konstantinos and Aravopoulou, Dionysia and Augsbach, Lukas and Sapper, Josef and Ottinger, Sarah and Psylla, Christina and Rafat, Ali Aghebat and Benitez-Montoya, Carlos Adrian and Miasnikova, Anna and Di, Zhenyu and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Kyritsis, Apostolos and Papadakis, Christine M.}, title = {Novel thermoresponsive block copolymers having different architectures-structural, rheological, thermal, and dielectric investigations}, series = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, volume = {292}, journal = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, number = {8}, publisher = {Springer}, address = {New York}, issn = {0303-402X}, doi = {10.1007/s00396-014-3282-0}, pages = {1757 -- 1774}, year = {2014}, abstract = {Thermoresponsive block copolymers comprising long, hydrophilic, nonionic poly(methoxy diethylene glycol acrylate) (PMDEGA) blocks and short hydrophobic polystyrene (PS) blocks are investigated in aqueous solution. Various architectures, namely diblock, triblock, and starblock copolymers are studied as well as a PMDEGA homopolymer as reference, over a wide concentration range. For specific characterization methods, polymers were labeled, either by partial deuteration (for neutron scattering studies) or by fluorophores. Using fluorescence correlation spectroscopy, critical micellization concentrations are identified and the hydrodynamic radii of the micelles, r (h) (mic) , are determined. Using dynamic light scattering, the behavior of r (h) (mic) in dependence on temperature and the cloud points are measured. Small-angle neutron scattering enabled the detailed structural investigation of the micelles and their aggregates below and above the cloud point. Viscosity measurements are carried out to determine the activation energies in dependence on the molecular architecture. Differential scanning calorimetry at high polymer concentration reveals the glass transition of the polymers, the fraction of uncrystallized water and effects of the phase transition at the cloud point. Dielectric relaxation spectroscopy shows that the polarization changes reversibly at the cloud point, which reflects the formation of large aggregates upon heating through the cloud point and their redissolution upon cooling.}, language = {en} } @article{KyriakosPhilippAdelsbergeretal.2014, author = {Kyriakos, Konstantinos and Philipp, Martine and Adelsberger, Joseph and Jaksch, Sebastian and Berezkin, Anatoly V. and Lugo, Dersy M. and Richtering, Walter and Grillo, Isabelle and Miasnikova, Anna and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Cononsolvency of water/methanol mixtures for PNIPAM and PS-b-PNIPAM: pathway of aggregate formation investigated using time-resolved SANS}, series = {Macromolecules : a publication of the American Chemical Society}, volume = {47}, journal = {Macromolecules : a publication of the American Chemical Society}, number = {19}, publisher = {American Chemical Society}, address = {Washington}, issn = {0024-9297}, doi = {10.1021/ma501434e}, pages = {6867 -- 6879}, year = {2014}, abstract = {We investigate the cononsolvency effect of poly(N-isopropylacrylamide) (PNIPAM) in mixtures of water and methanol. Two systems are studied: micellar solutions of polystyrene-b-poly(N-isopropylacrylamide) (PS-b-PNIPAM) diblock copolymers and, as a reference, solutions of PNIPAM homopolymers, both at a concentration of 20 mg/mL in DO. Using a stopped-flow instrument, fully deuterated methanol was rapidly added to these solutions at volume fractions between 10 and 20\%. Time-resolved turbidimetry revealed aggregate formation within 10-100 s. The structural changes on mesoscopic length scales were followed by time-resolved small-angle neutron scattering (TR-SANS) with a time resolution of 0.1 s. In both systems, the pathway of the aggregation depends on the content of deuterated methanol; however, it is fundamentally different for homopolymer and diblock copolymer solutions: In the former, very large aggregates (>150 nm) are formed within the dead time of the setup, gradient appears at their surface in the late stages. In contrast, the growth of the aggregates in the latter system features different regimes, and the final aggregate size is 50 nm, thus much smaller than for the homopolymer. For the diblock copolymer, the time dependence of the aggregate radius can be described by two models: In the initial stage, the diffusion-limited coalescence model describes the data well; however, the resulting coalescence time is unreasonably high. In the late stage, a logarithmic coalescence model based on an energy barrier which is proportional to the aggregate radius is successfully applied. and a concentration}, language = {en} } @article{AdelsbergerBivigouKoumbaMiasnikovaetal.2015, author = {Adelsberger, Joseph and Bivigou Koumba, Achille Mayelle and Miasnikova, Anna and Busch, Peter and Laschewsky, Andr{\´e} and M{\"u}ller-Buschbaum, Peter and Papadakis, Christine M.}, title = {Polystyrene-block-poly (methoxy diethylene glycol acrylate)-block-polystyrene triblock copolymers in aqueous solution-a SANS study of the temperature-induced switching behavior}, series = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, volume = {293}, journal = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, number = {5}, publisher = {Springer}, address = {New York}, issn = {0303-402X}, doi = {10.1007/s00396-015-3535-6}, pages = {1515 -- 1523}, year = {2015}, abstract = {A concentrated solution of a symmetric triblock copolymer with a thermoresponsive poly(methoxy diethylene glycol acrylate) (PMDEGA) middle block and short hydrophobic, fully deuterated polystyrene end blocks is investigated in D2O where it undergoes a lower critical solution temperature-type phase transition at ca. 36 A degrees C. Small-angle neutron scattering (SANS) in a wide temperature range (15-50 A degrees C) is used to characterize the size and inner structure of the micelles as well as the correlation between the micelles and the formation of aggregates by the micelles above the cloud point (CP). A model featuring spherical core-shell micelles, which are correlated by a hard-sphere potential or a sticky hard-sphere potential together with a Guinier form factor describing aggregates formed by the micelles above the CP, fits the SANS curves well in the entire temperature range. The thickness of the thermoresponsive micellar PMDEGA shell as well as the hard-sphere radius increase slightly already below the cloud point. Whereas the thickness of the thermoresponsive micellar shell hardly shrinks when heating through the CP and up to 50 A degrees C, the hard-sphere radius decreases within 3.5 K at the CP. The volume fraction decreases already significantly below the CP, which may be at the origin of the previously observed gel-sol transition far below the CP (Miasnikova et al., Langmuir 28: 4479-4490, 2012). Above the CP, small, and at higher temperatures, large aggregates are formed by the micelles.}, language = {en} } @article{ZhongWangAdelsbergeretal.2011, author = {Zhong, Qi and Wang, Weinan and Adelsberger, Joseph and Golosova, Anastasia and Koumba, Achille M. Bivigou and Laschewsky, Andr{\´e} and Funari, Sergio S. and Perlich, Jan and Roth, Stephan V. and Papadakis, Christine M. and M{\"u}ller-Buschbaum, Peter}, title = {Collapse transition in thin films of poly(methoxydiethylenglycol acrylate)}, series = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, volume = {289}, journal = {Colloid and polymer science : official journal of the Kolloid-Gesellschaft}, number = {5-6}, publisher = {Springer}, address = {New York}, issn = {0303-402X}, doi = {10.1007/s00396-011-2384-1}, pages = {569 -- 581}, year = {2011}, abstract = {The thermal behavior of poly(methoxydiethylenglycol acrylate) (PMDEGA) is studied in thin hydrogel films on solid supports and is compared with the behavior in aqueous solution. The PMDEGA hydrogel film thickness is varied from 2 to 422 nm. Initially, these films are homogenous, as measured with optical microscopy, atomic force microscopy, X-ray reflectivity, and grazing-incidence small-angle X-ray scattering (GISAXS). However, they tend to de-wet when stored under ambient conditions. Along the surface normal, no long-ranged correlations between substrate and film surface are detected with GISAXS, due to the high mobility of the polymer at room temperature. The swelling of the hydrogel films as a function of the water vapor pressure and the temperature are probed for saturated water vapor pressures between 2,380 and 3,170 Pa. While the swelling capability is found to increase with water vapor pressure, swelling in dependence on the temperature revealed a collapse phase transition of a lower critical solution temperature type. The transition temperature decreases from 40.6 A degrees C to 36.6 A degrees C with increasing film thickness, but is independent of the thickness for very thin films below a thickness of 40 nm. The observed transition temperature range compares well with the cloud points observed in dilute (0.1 wt.\%) and semi-dilute (5 wt.\%) solution which decrease from 45 A degrees C to 39 A degrees C with increasing concentration.}, language = {en} }