Investigation of thin films made from silicon-containing poly(phenylquinoxaline-amide)s

  • Thin films in the range of 50 nm to 10 mm thickness have been prepared from NMP solutions of silicon-containing polyphenylquinoxaline-amides which had been synthesized by the polycondensation reaction of aromatic diaminophenylquinoxalines with bis(p-chlorocarbonylphenyl)diphenylsilane. A spin-coating technique onto glass plates or onto silicon wafers was used to make the film, followed by gradual heating to remove the solvent. The resulting films were very smooth and free of pinholes when studied by atomic force microscopy (AFM). They showed a strong adhesion to silicon wafers, were thermally stable in air to above 400 °C and their dielectric constant was in the range of 3.5-3.7. Thermal treatment of the films was performed in order to induce crosslinking. Such treated films became completely insoluble in organic solvents, maintained their smoothness and strong adhesion to the silicon substrate, and did not show any Tg, in DSC experiments. Their FTIR spectra in reflection mode did not show any changes compared with the untreatedThin films in the range of 50 nm to 10 mm thickness have been prepared from NMP solutions of silicon-containing polyphenylquinoxaline-amides which had been synthesized by the polycondensation reaction of aromatic diaminophenylquinoxalines with bis(p-chlorocarbonylphenyl)diphenylsilane. A spin-coating technique onto glass plates or onto silicon wafers was used to make the film, followed by gradual heating to remove the solvent. The resulting films were very smooth and free of pinholes when studied by atomic force microscopy (AFM). They showed a strong adhesion to silicon wafers, were thermally stable in air to above 400 °C and their dielectric constant was in the range of 3.5-3.7. Thermal treatment of the films was performed in order to induce crosslinking. Such treated films became completely insoluble in organic solvents, maintained their smoothness and strong adhesion to the silicon substrate, and did not show any Tg, in DSC experiments. Their FTIR spectra in reflection mode did not show any changes compared with the untreated films, meaning on the one hand that the polymers maintain their structural integrity at high temperature and on the other hand that the number of crosslinks was very low and could not be detected by IR spectroscopy.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Suche bei Google Scholar Statistik - Anzahl der Zugriffe auf das Dokument
Metadaten
Verfasserangaben:Maria Bruma, Burkhard SchulzORCiDGND, Thomas Köpnick, Reinhard Dietel, Burkhard Stiller, Frank W. Mercer
Publikationstyp:Wissenschaftlicher Artikel
Sprache:Englisch
Jahr der Erstveröffentlichung:1998
Erscheinungsjahr:1998
Datum der Freischaltung:24.03.2017
Quelle:High performance polymers. - 10 (1998), S. 207 - 215