Characterization of Langmuir films prepared from copolyesterurethanes based on oligo(omega-pentadecalactone) and oligo(epsilon-caprolactone)segments

  • A series of multiblock copolymers (PDLCL) synthesized from oligo(omega-pentadecalactone) diol (OPDL) and oligo(epsilon-caprolactone) diol (OCL), which are linked by 2,2(4), 4-trimethyl-hexamethylene diisocyanate (TMDI), is investigated by the Langmuir monolayer technique at the air-water interface. Brewster angle microscopy (BAM) and spectroscopic ellipsometry are employed to characterize the polymer film morphologies in situ. PDLCL containing >= 40 wt% OCL segments form homogeneous Langmuir monofilms after spreading. The film elasticity modulus decreases with increasing amounts of OPDL segments in the copolymer. In contrast, the OCL-free polyesterurethane OPDL-TMDI cannot be spread to monomolecular films on the water surface properly, and movable slabs are observed by BAM even at low surface pressures. The results of the in situ morphological characterization clearly show that essential information concerning the reliability of Langmuir monolayer degradation (LMD) experiments cannot be obtained from the evaluation of the pi-AA series of multiblock copolymers (PDLCL) synthesized from oligo(omega-pentadecalactone) diol (OPDL) and oligo(epsilon-caprolactone) diol (OCL), which are linked by 2,2(4), 4-trimethyl-hexamethylene diisocyanate (TMDI), is investigated by the Langmuir monolayer technique at the air-water interface. Brewster angle microscopy (BAM) and spectroscopic ellipsometry are employed to characterize the polymer film morphologies in situ. PDLCL containing >= 40 wt% OCL segments form homogeneous Langmuir monofilms after spreading. The film elasticity modulus decreases with increasing amounts of OPDL segments in the copolymer. In contrast, the OCL-free polyesterurethane OPDL-TMDI cannot be spread to monomolecular films on the water surface properly, and movable slabs are observed by BAM even at low surface pressures. The results of the in situ morphological characterization clearly show that essential information concerning the reliability of Langmuir monolayer degradation (LMD) experiments cannot be obtained from the evaluation of the pi-A isotherms only. Consequently, in situ morphological characterization turns out to be indispensable for characterization of Langmuir layers before LMD experiments.show moreshow less

Export metadata

Additional Services

Search Google Scholar Statistics
Metadaten
Author details:Anne-Christin SchöneGND, Burkhard SchulzORCiDGND, Klaus Richau, Karl KratzORCiD, Andreas LendleinORCiDGND
DOI:https://doi.org/10.1002/macp.201400377
ISSN:1022-1352
ISSN:1521-3935
Title of parent work (English):Macromolecular chemistry and physics
Publisher:Wiley-VCH
Place of publishing:Weinheim
Publication type:Article
Language:English
Year of first publication:2014
Publication year:2014
Release date:2017/03/27
Tag:Langmuir layers; brewster angle microscopy; ellipsometry; morphology; polyesterurethanes
Volume:215
Issue:24
Number of pages:9
First page:2437
Last Page:2445
Organizational units:Mathematisch-Naturwissenschaftliche Fakultät / Institut für Chemie
Peer review:Referiert
Accept ✔
This website uses technically necessary session cookies. By continuing to use the website, you agree to this. You can find our privacy policy here.