TY - JOUR A1 - Bruma, Maria A1 - Sava, Ion A1 - Mercer, Frank W. A1 - Reddy, Victor N. A1 - Köpnick, Thomas A1 - Stiller, Burkhard A1 - Schulz, Burkhard T1 - Silicon-containing poly(amide-ether)s N2 - New aromatic poly(amide-ether)s (II) have been synthesized by solution polycondensation of various aromatic diamines having two ether bridges (I) with a diacid chloride containing silicon, namely bis(chlorocarbonylphenyl)- diphenyIsilane. These polymers are easy soluble in polar amidic solvents such as N-methylpyrrolidinone or dimethylformamide and can be cast into thin flexible films or coatings from such solutions. They show high thermal stability with initial decomposition temperature being above 400 °C. Their glass transition temperatures lie in the range of 220-250 °C, except for polymer He which did not show a clear Tg when heated in a differential scanning calorimetry experiment up to 300 °C. The large interval between the glass transition and decomposition temperatures of pnlymers Ia-Id could be advantageous for their processing via compression molding. The polymer coatings deposited by the spincoating, technique onto silicon wafers showed a very smooth, pinhole-free surface in atomic force microscopy investigations. The free-standing films of 20-30 mm thickness show low dielectric constant, in the range of 3.65-3.78, which is promising for future application as high performance dielectrics. Y1 - 1998 ER -