TY - THES A1 - Behrendt, Felix Nicolas T1 - New bio-based polymers T1 - Neue biobasierte Polymere BT - synthesis and polymerization of cystine-based macrocycles BT - Synthese und Polymerisation von cystinbasierten Makrozyklen N2 - Redox-responsive polymers, such as poly(disulfide)s, are a versatile class of polymers with potential applications including gene- and drug-carrier systems. Their degradability under reductive conditions allows for a controlled response to the different redox states that are present throughout the body. Poly(disulfide)s are typically synthesized by step growth polymerizations. Step growth polymerizations, however, may suffer from low conversions and therefore low molar masses, limiting potential applications. The purpose of this thesis was therefore to find and investigate new synthetic routes towards the synthesis of amino acid-based poly(disulfide)s. The different routes in this thesis include entropy-driven ring opening polymerizations of novel macrocyclic monomers, derived from cystine derivatives. These monomers were obtained with overall yields of up to 77% and were analyzed by mass spectrometry as well as by 1D and 2D NMR spectroscopy. The kinetics of the entropy-driven ring-opening metathesis polymerization (ED-ROMP) were thoroughly investigated in dependence of temperature, monomer concentration, and catalyst concentration. The polymerization was optimized to yield poly(disulfide)s with weight average molar masses of up to 80 kDa and conversions of ~80%, at the thermodynamic equilibrium. Additionally, an alternative metal free polymerization, namely the entropy-driven ring-opening disulfide metathesis polymerization (ED-RODiMP) was established for the polymerization of the macrocyclic monomers. The effect of different solvents, concentrations and catalyst loadings on the polymerization process and its kinetics were studied. Polymers with very high weight average molar masses of up to 177 kDa were obtained. Moreover, various post-polymerization reactions were successfully performed. This work provides the first example of the homopolymerization of endo-cyclic disulfides by ED-ROMP and the first substantial study into the kinetics of the ED-RODiMP process. N2 - Redoxresponsive Polymere, wie etwa Polydisulfide, sind eine vielseitige Klasse von Polymeren, die unter anderem als Gen- und Wirkstoffträgersysteme eingesetzt werden können. Ihre Abbaubarkeit unter reduktiven Bedingungen ermöglicht eine kontrollierte Reaktion auf die verschiedenen Redoxzustände im Körper. Polydisulfide werden jedoch häufig durch Stufenwachstums-polymerisationen synthetisiert. Diese führen oft zu niedrigen Umsätzen und daher zu niedrigen molaren Massen. Das Ziel dieser Arbeit war daher neue Synthesewege für aminosäurebasierte Polydisulfide zu finden und zu untersuchen. Diese Wege beinhalteten entropiegetriebene ringöffnende Polymerisationen von neuen makrozyklischen Monomeren, auf der Basis von Cystin-Derivaten. Diese Monomere konnten mit einer Gesamtausbeute von bis zu 77% synthetisiert werden und wurden mit Massenspektrometrie sowie mit 1D- und 2D-NMR-Spektroskopie analysiert. Die Kinetik der entropiegetriebenen ringöffnenden Metathese Polymerisation (ED-ROMP) wurde im Hinblick auf Temperatur, Monomerkonzentration und Katalysatormenge sorgfältig untersucht. Durch Optimierungen konnten Polydisulfide mit gewichtsmittleren Molmassen von bis zu 80 kDa und Umsätzen von ~80%, im thermodynamischen Gleichgewicht synthetisiert werden. Zusätzlich wurde eine alternative metallfreie Polymerisation, die entropiegetriebene ringöffnende Disulfidmetathese Polymerisation (ED-RODiMP), für die Polymerisation der makrozyklischen Monomere etabliert. Die Auswirkungen verschiedener Lösungsmittel, Konzentrationen und Katalysatorkonzentrationen auf die Kinetik dieses Polymerisationsprozesses wurden untersucht. Hierdurch wurden Polymere mit sehr hohen gewichtsmittleren Molmassen von bis zu 177 kDa erhalten. Darüber hinaus wurden verschiedene Postpolymerisationsreaktionen erfolgreich durchgeführt. Diese Arbeit liefert das erste Beispiel für die Homopolymerisation endo-zyklischer Disulfide durch ROMP und eine erste substanzielle Studie der Kinetik des ED-RODiMP-Prozesses. KW - polymers KW - ADMET KW - ROMP KW - disulfide KW - macrocycles KW - ring-opening polymerization KW - amino acids KW - Polymere KW - ADMET KW - ROMP KW - Disulfide KW - Makrozyklen KW - ringöffnende Polymerisation KW - Aminosäuren Y1 - 2018 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:517-opus4-418316 ER - TY - THES A1 - Debsharma, Tapas T1 - Cellulose derived polymers T1 - Polymere aus Cellulose BT - synthesis of functional and degradable polymers from cellulose N2 - Plastics, such as polyethylene, polypropylene, and polyethylene terephthalate are part of our everyday lives in the form of packaging, household goods, electrical insulation, etc. These polymers are non-degradable and create many environmental problems and public health concerns. Additionally, these polymers are produced from finite fossils resources. With the continuous utilization of these limited resources, it is important to look towards renewable sources along with biodegradation of the produced polymers, ideally. Although many bio-based polymers are known, such as polylactic acid, polybutylene succinate adipate or polybutylene succinate, none have yet shown the promise of replacing conventional polymers like polyethylene, polypropylene and polyethylene terephthalate. Cellulose is one of the most abundant renewable resources produced in nature. It can be transformed into various small molecules, such as sugars, furans, and levoglucosenone. The aim of this research is to use the cellulose derived molecules for the synthesis of polymers. Acid-treated cellulose was subjected to thermal pyrolysis to obtain levoglucosenone, which was reduced to levoglucosenol. Levoglucosenol was polymerized, for the first time, by ring-opening metathesis polymerization (ROMP) yielding high molar mass polymers of up to ~150 kg/mol. The poly(levoglucosenol) is thermally stable up to ~220 ℃, amorphous, and is exhibiting a relatively high glass transition temperature of ~100 ℃. The poly(levoglucosenol) can be converted to a transparent film, resembling common plastic, and was found to degrade in a moist acidic environment. This means that poly(levoglucosenol) may find its use as an alternative to conventional plastic, for instance, polystyrene. Levoglucosenol was also converted into levoglucosenyl methyl ether, which was polymerized by cationic ring-opening metathesis polymerization (CROP). Polymers were obtained with molar masses up to ~36 kg/mol. These polymers are thermally stable up to ~220 ℃ and are semi-crystalline thermoplastics, having a glass transition temperature of ~35 ℃ and melting transition of 70-100 ℃. Additionally, the polymers underwent cross-linking, hydrogenation and thiol-ene click chemistry. N2 - Kunststoffe wie Polyethylen, Polypropylen und Polyethylenterephthalat sind ein großer Bestandteil unseres Alltags und finden Verwendung unter anderem als Verpackungsmaterialien, Haushaltswaren und Elektroisolierungen. Diese Polymere werden aus fossilen Ressourcen hergestellt, sind nicht abbaubar und verursachen nicht nur viele Umweltprobleme sondern können auch zu Gesundheitsschäden führen. Aufgrund dessen muss die Verwendung von erneuerbaren Ressourcen geachtet werden, wobei die hergestellten Polymere im Idealfall komplett biologisch abbaubar sind. Obwohl viele biobasierte Polymere, wie Polymilchsäure, Polybutylensuccinatadipat oder Polybutylensuccinat, bekannt sind, hat noch keines das Potential gezeigt, herkömmliche Polymere zu ersetzen. Cellulose ist einer der am häufigsten in der Natur produzierten nachwachsenden Rohstoffe und kann in verschiedene kleine organische Moleküle wie Zucker (Saccharide), Furan und auch Levoglucosenon umgewandelt werden. Ziel dieser Arbeit ist die Verwendung von Levoglucosenon als Monomer für die Synthese von Polymeren. Säurebehandelte Cellulose wurde einer thermischen Pyrolyse unterzogen, um Levoglucosenon zu erhalten, das dann weiter zu Levoglucosenol reduziert wurde. Das Levoglucosenol wurde zum ersten Mal erfolgreich über eine Ringöffnungsmetathese-Polymerisation (ROMP) polymerisiert. Die Molmassen der hergestellten Polymere erreichten Werte von bis zu ~150 kg/mol. Die thermische Analyse von Poly(levoglucosenol) zeigt, dass es bis zu einer Temperatur von ~220 ℃ stabil ist, eine Glasübergangstemperatur bei ~100 ℃ hat und ein amorphes Polymer ist. Weiterhin kann das Poly(levoglucosenol) in feuchter saurer Umgebung in kurzer Zeit abgebaut werden. Aufgrund dieser Eigenschaften kann Poly(levoglucosenol) als Alternative zu konventionellem Kunststoff, wie z.B. Polystyrol, eingesetzt werden kann. Levoglucosenol wurde weiter in Levoglucosenylmethylether umgewandelt. Levoglucosenylmethylether kann mit kationischer Ringöffnungs-Polymerisation (CROP) polymerisiert werden. Es wurden Polymere mit Molmassen von bis zu ~36 kg/mol hergestellt. Die Polymere weisen eine thermische Stabilität bis zu einer Temperatur von ~220 °C auf. Es handelt sich bei den hergestellten Poly(levoglucosenylmethylethern) um teilkristalline Thermoplaste, deren Glasüberganstemperatur bei ~35 °C und der Schmelzbereich bei 70-100 °C liegt. Die Doppelbindungen des Levoglucosenylmethylethers wurden genutzt um das Polymer zu vernetzen und zu funktionalisieren. KW - biomass valorization KW - levoglucosenol KW - ring-opening polymerization KW - degradable polymer KW - sustainable chemistry KW - Biomasseverwertung KW - Levoglucosenol KW - ringöffnende Polymerisation KW - abbaubares Polymer KW - nachhaltige Chemie Y1 - 2019 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:517-opus4-441312 ER -