TY - JOUR A1 - Nizardo, Noverra M. A1 - Schanzenbach, Dirk A1 - Schönemann, Eric A1 - Laschewsky, Andre T1 - Exploring poly(ethylene glycol)-polyzwitterion diblock copolymers as biocompatible smart macrosurfactants featuring UCST-phase behavior in normal saline solution JF - Polymers N2 - Nonionic-zwitterionic diblock copolymers are designed to feature a coil-to-globule collapse transition with an upper critical solution temperature (UCST) in aqueous media, including physiological saline solution. The block copolymers that combine presumably highly biocompatible blocks are synthesized by chain extension of a poly(ethylene glycol) (PEG) macroinitiator via atom transfer radical polymerization (ATRP) of sulfobetaine and sulfabetaine methacrylates. Their thermoresponsive behavior is studied by variable temperature turbidimetry and H-1 NMR spectroscopy. While the polymers with polysulfobetaine blocks exhibit phase transitions in the physiologically interesting window of 30-50 degrees C only in pure aqueous solution, the polymers bearing polysulfabetaine blocks enabled phase transitions only in physiological saline solution. By copolymerizing a pair of structurally closely related sulfo-and sulfabetaine monomers, thermoresponsive behavior can be implemented in aqueous solutions of both low and high salinity. Surprisingly, the presence of the PEG blocks can affect the UCST-transitions of the polyzwitterions notably. In specific cases, this results in "schizophrenic" thermoresponsive behavior displaying simultaneously an UCST and an LCST (lower critical solution temperature) transition. Exploratory experiments on the UCST-transition triggered the encapsulation and release of various solvatochromic fluorescent dyes as model "cargos" failed, apparently due to the poor affinity even of charged organic compounds to the collapsed state of the polyzwitterions. KW - block copolymer KW - amphiphile KW - macrosurfactant KW - thermoresponsive self-assembly KW - polyzwitterion KW - upper critical solution temperature (UCST) KW - salting-in Y1 - 2018 U6 - https://doi.org/10.3390/polym10030325 SN - 2073-4360 VL - 10 IS - 3 PB - MDPI CY - Basel ER - TY - GEN A1 - Schönemann, Eric A1 - Laschewsky, André A1 - Rosenhahn, Axel T1 - Exploring the long-term hydrolytic behavior of zwitterionic polymethacrylates and polymethacrylamides T2 - Postprints der Universität Potsdam : Mathematisch-Naturwissenschaftliche Reihe N2 - The hydrolytic stability of polymers to be used for coatings in aqueous environments, for example, to confer anti-fouling properties, is crucial. However, long-term exposure studies on such polymers are virtually missing. In this context, we synthesized a set of nine polymers that are typically used for low-fouling coatings, comprising the well-established poly(oligoethylene glycol methylether methacrylate), poly(3-(N-2-methacryloylethyl-N,N-dimethyl) ammoniopropanesulfonate) (“sulfobetaine methacrylate”), and poly(3-(N-3-methacryamidopropyl-N,N-dimethyl)ammoniopropanesulfonate) (“sulfobetaine methacrylamide”) as well as a series of hitherto rarely studied polysulfabetaines, which had been suggested to be particularly hydrolysis-stable. Hydrolysis resistance upon extended storage in aqueous solution is followed by ¹H NMR at ambient temperature in various pH regimes. Whereas the monomers suffered slow (in PBS) to very fast hydrolysis (in 1 M NaOH), the polymers, including the polymethacrylates, proved to be highly stable. No degradation of the carboxyl ester or amide was observed after one year in PBS, 1 M HCl, or in sodium carbonate buffer of pH 10. This demonstrates their basic suitability for anti-fouling applications. Poly(sulfobetaine methacrylamide) proved even to be stable for one year in 1 M NaOH without any signs of degradation. The stability is ascribed to a steric shielding effect. The hemisulfate group in the polysulfabetaines, however, was found to be partially labile. T3 - Zweitveröffentlichungen der Universität Potsdam : Mathematisch-Naturwissenschaftliche Reihe - 1091 KW - polyzwitterions KW - stability KW - polymer degradation KW - hydrolysis KW - polysulfobetaine KW - polysulfabetaine KW - anti-fouling materials Y1 - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:517-opus4-473052 SN - 1866-8372 IS - 1091 ER - TY - JOUR A1 - Schönemann, Eric A1 - Laschewsky, Andre A1 - Rosenhahn, Axel T1 - Exploring the long-term hydrolytic behavior of zwitterionic polymethacrylates and polymethacrylamides JF - Polymers N2 - The hydrolytic stability of polymers to be used for coatings in aqueous environments, for example, to confer anti-fouling properties, is crucial. However, long-term exposure studies on such polymers are virtually missing. In this context, we synthesized a set of nine polymers that are typically used for low-fouling coatings, comprising the well-established poly(oligoethylene glycol methylether methacrylate), poly(3-(N-2-methacryloylethyl-N,N-dimethyl) ammoniopropanesulfonate) (sulfobetaine methacrylate), and poly(3-(N-3-methacryamidopropyl-N,N-dimethyl)ammoniopropanesulfonate) (sulfobetaine methacrylamide) as well as a series of hitherto rarely studied polysulfabetaines, which had been suggested to be particularly hydrolysis-stable. Hydrolysis resistance upon extended storage in aqueous solution is followed by H-1 NMR at ambient temperature in various pH regimes. Whereas the monomers suffered slow (in PBS) to very fast hydrolysis (in 1 M NaOH), the polymers, including the polymethacrylates, proved to be highly stable. No degradation of the carboxyl ester or amide was observed after one year in PBS, 1 M HCl, or in sodium carbonate buffer of pH 10. This demonstrates their basic suitability for anti-fouling applications. Poly(sulfobetaine methacrylamide) proved even to be stable for one year in 1 M NaOH without any signs of degradation. The stability is ascribed to a steric shielding effect. The hemisulfate group in the polysulfabetaines, however, was found to be partially labile. KW - polyzwitterions KW - stability KW - polymer degradation KW - hydrolysis KW - polysulfobetaine KW - polysulfabetaine KW - anti-fouling materials Y1 - 2018 U6 - https://doi.org/10.3390/polym10060639 SN - 2073-4360 VL - 10 IS - 6 PB - MDPI CY - Basel ER -