@article{NeffeLoewenbergJulichGruneretal.2021, author = {Neffe, Axel T. and L{\"o}wenberg, Candy and Julich-Gruner, Konstanze K. and Behl, Marc and Lendlein, Andreas}, title = {Thermally-induced shape-memory behavior of degradable gelatin-based networks}, series = {International journal of molecular sciences}, volume = {22}, journal = {International journal of molecular sciences}, number = {11}, publisher = {Molecular Diversity Preservation International}, address = {Basel}, issn = {1422-0067}, doi = {10.3390/ijms22115892}, pages = {15}, year = {2021}, abstract = {Shape-memory hydrogels (SMH) are multifunctional, actively-moving polymers of interest in biomedicine. In loosely crosslinked polymer networks, gelatin chains may form triple helices, which can act as temporary net points in SMH, depending on the presence of salts. Here, we show programming and initiation of the shape-memory effect of such networks based on a thermomechanical process compatible with the physiological environment. The SMH were synthesized by reaction of glycidylmethacrylated gelatin with oligo(ethylene glycol) (OEG) alpha,omega-dithiols of varying crosslinker length and amount. Triple helicalization of gelatin chains is shown directly by wide-angle X-ray scattering and indirectly via the mechanical behavior at different temperatures. The ability to form triple helices increased with the molar mass of the crosslinker. Hydrogels had storage moduli of 0.27-23 kPa and Young's moduli of 215-360 kPa at 4 degrees C. The hydrogels were hydrolytically degradable, with full degradation to water-soluble products within one week at 37 degrees C and pH = 7.4. A thermally-induced shape-memory effect is demonstrated in bending as well as in compression tests, in which shape recovery with excellent shape-recovery rates R-r close to 100\% were observed. In the future, the material presented here could be applied, e.g., as self-anchoring devices mechanically resembling the extracellular matrix.}, language = {en} } @article{NeffeLoewenbergLendlein2021, author = {Neffe, Axel T. and L{\"o}wenberg, Candy and Lendlein, Andreas}, title = {Hydrogel networks by aliphatic dithiol Michael addition to glycidylmethacrylated gelatin}, series = {MRS advances : a journal of the Materials Research Society (MRS)}, volume = {6}, journal = {MRS advances : a journal of the Materials Research Society (MRS)}, number = {33}, publisher = {Springer Nature Switzerland AG}, address = {Cham}, issn = {2059-8521}, doi = {10.1557/s43580-021-00136-8}, pages = {796 -- 800}, year = {2021}, abstract = {Functionalization of gelatin with glycidylmethacrylate (GMA-gelatin) enables network formation employing the double bond, so that the reaction is orthogonal to the inherent functional groups in the biomacromolecule. Here, network formation by crosslinking of GMA-gelatin with hexane 1,6-dithiol or nonane 1,9-dithiol to tailor properties and enable a shape-memory effect is shown by H-1 NMR and FT-IR spectroscopy. Hydrogel swelling (460-1900 vol\%) and mechanical properties (Young's modulus E = 59-512 kPa, elongation at break epsilon(b) = 44-127\%) depended on the molecular composition of the networks and temperature. Increased crosslinker length, thiol:methacrylate molar ratio, and precursor concentrations led to denser networks. Change of properties with temperature suggested adoption of triple helices by gelatin chains, forming physical netpoints at lower temperatures (< 20 degrees C). However, the limited freedom of the gelatin chains to move allowed only a minimal extent of triple helices formation, as it became apparent from the related signal in wide-angle X-ray scattering and the thermal transition associated to triple helices in some networks by DSC. The presented strategy is likely transferable to other biomacromolecules, and the results suggest that too short crosslinkers may result in a significant amount of grafting rather than network formation.}, language = {en} } @article{NeffeIzraylitHommesSchattmannetal.2021, author = {Neffe, Axel T. and Izraylit, Victor and Hommes-Schattmann, Paul J. and Lendlein, Andreas}, title = {Soft, formstable (Co)polyester blend elastomers}, series = {Nanomaterials : open access journal}, volume = {11}, journal = {Nanomaterials : open access journal}, number = {6}, publisher = {MDPI}, address = {Basel}, issn = {2079-4991}, doi = {10.3390/nano11061472}, pages = {18}, year = {2021}, abstract = {High crystallization rate and thermomechanical stability make polylactide stereocomplexes effective nanosized physical netpoints. Here, we address the need for soft, form-stable degradable elastomers for medical applications by designing such blends from (co)polyesters, whose mechanical properties are ruled by their nanodimensional architecture and which are applied as single components in implants. By careful controlling of the copolymer composition and sequence structure of poly[(L-lactide)-co-(epsilon-caprolactone)], it is possible to prepare hyperelastic polymer blends formed through stereocomplexation by adding poly(D-lactide) (PDLA). Low glass transition temperature T-g <= 0 degrees C of the mixed amorphous phase contributes to the low Young's modulus E. The formation of stereocomplexes is shown in DSC by melting transitions T-m > 190 degrees C and in WAXS by distinct scattering maxima at 2 theta = 12 degrees and 21 degrees. Tensile testing demonstrated that the blends are soft (E = 12-80 MPa) and show an excellent hyperelastic recovery R-rec = 66-85\% while having high elongation at break epsilon(b) up to >1000\%. These properties of the blends are attained only when the copolymer has 56-62 wt\% lactide content, a weight average molar mass >140 kg center dot mol(-1), and number average lactide sequence length >= 4.8, while the blend is formed with a content of 5-10 wt\% of PDLA. The devised strategy to identify a suitable copolymer for stereocomplexation and blend formation is transferable to further polymer systems and will support the development of thermoplastic elastomers suitable for medical applications.}, language = {en} } @article{NeffeZhangHommesSchattmannetal.2021, author = {Neffe, Axel T. and Zhang, Quanchao and Hommes-Schattmann, Paul J. and Lendlein, Andreas}, title = {Ethylene oxide sterilization of electrospun poly(L-lactide)/poly(D-lactide) core/shell nanofibers}, series = {MRS advances}, volume = {6}, journal = {MRS advances}, number = {33}, publisher = {Springer}, address = {Cham}, issn = {2059-8521}, doi = {10.1557/s43580-021-00058-5}, pages = {786 -- 789}, year = {2021}, abstract = {The application of polymers in medicine requires sterilization while retaining material structure and properties. This demands detailed analysis, which we show exemplarily for the sterilization of PLLA/PDLA core-shell nanofibers with ethylene oxide (EtO). The electrospun patch was exposed to EtO gas (6 vol\% in CO2, 1.7 bar) for 3 h at 45 degrees C and 75\% rel. humidity, followed by degassing under pressure/vacuum cycles for 12 h. GC-MS analysis showed that no residual EtO was retained. Fiber diameters (similar to 520 +/- 130 nm) of the patches remained constant as observed by electron microscopy. Young's modulus slightly increased and the elongation at break slightly decreased, determined at 37 degrees C. No changes were detected in H-1-NMR spectra, in molar mass distribution (GPC) or in crystallinity measured for annealed samples with comparable thermal history (Wide Angle X-Ray Scattering). Altogether, EtO emerged as suitable sterilization method for polylactide nanofibers with core-shell morphology.}, language = {en} }