@phdthesis{Heinz2024, author = {Heinz, Markus}, title = {Synthese von Monomeren auf der Basis nachwachsender Rohstoffe und ihre Polymerisation}, doi = {10.25932/publishup-63794}, url = {http://nbn-resolving.de/urn:nbn:de:kobv:517-opus4-637943}, school = {Universit{\"a}t Potsdam}, pages = {XVII, 267}, year = {2024}, abstract = {Die vorliegende Arbeit thematisiert die Synthese und die Polymerisation von Monomeren auf der Basis nachwachsender Rohstoffe wie zum Beispiel in Gew{\"u}rzen und ätherischen Ölen enthaltenen kommerziell verf{\"u}gbaren Phenylpropanoiden (Eugenol, Isoeugenol, Zimtalkohol, Anethol und Estragol) und des Terpenoids Myrtenol sowie ausgehend von der Rinde einer Birke (Betula pendula) und der Korkeiche (Quercus suber). Ausgew{\"a}hlte Phenylpropanoide (Eugenol, Isoeugenol und Zimtalkohol) und das Terpenoid Myrtenol wurden zun{\"a}chst in den jeweiligen Laurylester {\"u}berf{\"u}hrt und anschließend das olefinische Strukturelement epoxidiert, wobei 4 neue (2-Methoxy-4-(oxiran-2-ylmethyl)phenyldodecanoat, 2-Methoxy-4-(3-methyl-oxiran-2-yl)phenyldodecanoat, (3-Phenyloxiran-2-yl)methyldodecanoat, (7,7-Dimethyl-3-oxatricyclo[4.1.1.02,4]octan-2-yl)methyldodecanoat) und 2 bereits bekannte monofunktionelle Epoxide (2-(4-Methoxybenzyl)oxiran und 2-(4-Methoxyphenyl)-3-methyloxiran) erhalten wurden, die mittels 1H-NMR-, 13C-NMR- und FT-IR-Spektroskopie sowie mit DSC untersucht wurden. Die Photo-DSC Untersuchung der Epoxidmonomere in einer kationischen Photopolymerisation bei 40 °C ergab die maximale Polymerisationsgeschwindigkeit (Rpmax: 0,005 s-1 bis 0,038 s-1) sowie die Zeit (tmax: 13 s bis 26 s) bis zum Erreichen des Rpmax-Wertes und f{\"u}hrte zu fl{\"u}ssigen Oligomeren, deren zahlenmittlerer Polymerisationsgrad mit 3 bis 6 mittels GPC bestimmt wurde. Die Umsetzung von 2-Methoxy-4-(oxiran-2-ylmethyl)phenyldodecanoat mit Methacrylsäure ergab ein Isomerengemisch (2-Methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat und 2-Methoxy-4-(2-(methacryl-oyloxy)-3-hydroxypropyl)phenyldodecanoat), das mittels Photo-DSC in einer freien radikalischen Photopolymerisation untersucht wurde (Rpmax: 0,105 s-1 und tmax: 5 s), die zu festen in Chloroform unlöslichen Polymeren f{\"u}hrte. Aus Korkpulver und gemahlener Birkenrinde wurden selektiv 2 kristalline ω-Hydroxyfettsäuren (9,10-Epoxy-18-hydroxyoctadecansäure und 22-Hydroxydocosansäure) isoliert. Die kationische Photopolymerisation der 9,10-Epoxy-18-hydroxyoctadecansäure ergab einen nahezu farblosen transparenten und bei Raumtemperatur elastischen Film, welcher ein Anwendungspotential f{\"u}r Oberflächenbeschichtungen hat. Aus der Reaktion von 9,10-Epoxy-18-hydroxyoctadecansäure mit Methacrylsäure wurde ein bei Raumtemperatur fl{\"u}ssiges Gemisch aus zwei Konstitutionsisomeren (9,18-Dihydroxy-10-(methacryloyloxy)octadecansäure und 9-(Methacryloyloxy)-10,18-dihydroxyoctadecansäure) erhalten (Tg: -60 °C). Die radikalische Photopolymerisation dieser Konstitutionsisomere wurde ebenfalls mittels Photo-DSC untersucht (Rpmax: 0,098 s-1 und tmax: 3,8 s). Die Reaktion von 22-Hydroxydocosansäure mit Methacryloylchlorid ergab die kristalline 22-(Methacryloyloxy)docosansäure, welche ebenfalls in einer radikalischen Photopolymerisation mittels Photo-DSC untersucht wurde (Rpmax: 0,023 s-1 und tmax: 9,6 s). Die mittels AIBN in Dimethylsulfoxid initiierte Homopolymerisation der 22-(Methacryloyloxy)docosansäure und der Isomerengemische bestehend aus 2-Methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat und 2-Methoxy-4-(2-(methacryl-oyloxy)-3-hydroxypropyl)phenyldodecanoat sowie aus 9,18-Dihydroxy-10-(methacryloy-loxy)octadecansäure und 9-(Methacryloyloxy)-10,18-dihydroxyoctadecansäure ergab feste lösliche Polymere, die mittels 1H-NMR- und FT-IR-Spektroskopie, GPC (Poly(2-methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat / 2-methoxy-4-(2-(methacryloyloxy)-3-hydroxypropyl)phenyldodecanoat): Pn = 94) und DSC (Poly(2-methoxy-4-(2-hydroxy-3-(methacryloyloxy)propyl)phenyldodecanoat / 2-methoxy-4-(2-(methacryloyloxy)-3-hydroxypropyl)phenyldodecanoat): Tg: 52 °C; Poly(9,18-dihydroxy-10-(methacryloyloxy)-octadecansäure / 9-(methacryloyloxy)-10,18-dihydroxyoctadecansäure): Tg: 10 °C; Poly(22-(methacryloyloxy)docosansäure): Tm: 74,1 °C, wobei der Schmelzpunkt mit dem des Photopolymers (Tm = 76,8 °C) vergleichbar ist) charakterisiert wurden. Das bereits bekannte Monomer 4-(4-Methacryloyloxyphenyl)butan-2-on wurde ausgehend von 4-(4-Hydroxyphenyl)butan-2-on hergestellt, welches aus Birkenrinde gewonnen werden kann, und unter identischen Bedingungen f{\"u}r einen Vergleich mit den neuen Monomeren polymerisiert. Die freie radikalische Polymerisation f{\"u}hrte zu Poly(4-(4-methacryloyloxyphenyl)butan-2-on) (Pn: 214 und Tg: 83 °C). Neben der Homopolymerisation wurde eine statistische Copolymerisation des Isomerengemisches 2-Methoxy-4-(2-hydroxy-3-(methacryl-oyloxy)propyl)phenyldodecanoat / 2-Methoxy-4-(2-(methacryloyloxy)-3-hydroxypropyl)-phenyldodecanoat mit 4-(4-Methacryloyloxyphenyl)butan-2-on untersucht, wobei ein äquimolarer Einsatz der Ausgangsmonomere zu einem Anstieg der Ausbeute, der Molmassenverteilung und der Dispersität des Copolymers (Tg: 44 °C) f{\"u}hrte. Die unter Verwendung von Diethylcarbonat als „gr{\"u}nes" Lösungsmittel mittels AIBN initiierten freien radikalischen Homopolymerisationen von 4-(4-Methacryloyloxyphenyl)butan-2-on und von Laurylmethacrylat ergaben vergleichbare Polymerisationsgrade der Homopolymere (Pn: 150), welche jedoch aufgrund ihrer Strukturunterschiede deutlich unterschiedliche Glas{\"u}bergangstemperaturen hatten (Poly(4-(4-methacryloyloxyphenyl)butan-2-on): Tg: 70 °C, Poly(laurylmethacrylat) Tg: -49 °C. Eine statistische Copolymerisation äquimolarer Stoffmengen der beiden Monomere in Diethylcarbonat f{\"u}hrte bei einer Polymerisationszeit von 60 Minuten zu einem leicht bevorzugten Einbau des 4-(4-Methacryloyloxyphenyl)butan-2-on in das Copolymer (Tg: 17 °C). Copolymerisationsdiagramme f{\"u}r die freien radikalischen Copolymerisationen von 4-(4-Methacryloyloxyphenyl)butan-2-on mit n-Butylmethacrylat beziehungsweise 2-(Dimethylamino)ethylmethacrylat (t: 20 min bis 60 min; Molenbr{\"u}che (X) f{\"u}r 4-(4-Methacryloyloxyphenyl)butan-2-on: 0,2; 0,4; 0,6 und 0,8) zeigten ein nahezu ideales azeotropes Copolymerisationsverhalten, obwohl ein leicht bevorzugter Einbau von 4-(4-Methacryloyloxyphenyl)butan-2-on in das jeweilige Copolymer beobachtet wurde. Dabei korreliert ein Anstieg der Ausbeute und der Glas{\"u}bergangstemperatur der erhaltenen Copolymere mit einem zunehmenden Gehalt an 4-(4-Methacryloyloxyphenyl)butan-2-on im Reaktionsgemisch. Die unter Einsatz der modifizierten Gibbs-DiMarzio-Gleichung berechneten Glas{\"u}bergangstemperaturen der Copolymere stimmten mit den gemessenen Werten gut {\"u}berein. Das ist eine gute Ausgangsbasis f{\"u}r die Bestimmung der Glas{\"u}bergangstemperatur eines Copolymers mit einer beliebigen Zusammensetzung.}, language = {de} } @phdthesis{Ilic2020, author = {Ilic, Ivan}, title = {Design of sustainable cathodes for Li-ion batteries}, doi = {10.25932/publishup-48368}, url = {http://nbn-resolving.de/urn:nbn:de:kobv:517-opus4-483689}, school = {Universit{\"a}t Potsdam}, pages = {iv, 154}, year = {2020}, abstract = {In recent years people have realised non-renewability of our modern society which relays on spending huge amounts of energy mostly produced from fosil fuels, such as oil and coal, and the shift towards more sustainable energy sources has started. However, sustainable sources of energy, such as wind-, solar- and hydro-energy, produce primarily electrical energy and can not just be poured in canister like many fosil fuels, creating necessity for rechragable batteries. However, modern Li-ion batteries are made from toxic heavy metals and sustainable alternatives are needed. Here we show that naturally abundant catecholic and guaiacyl groups can be utilised to replace heavy metals in Li-ion batteries. Foremost vanillin, a naturally occurring food additive that can be sustainably synthesised from industrial biowaste, lignin, was utilised to synthesise materials that showed extraordinary performance as cathodes in Li-ion batteries. Furthermore, behaviour of catecholic and guiacyl groups in Li-ion system was compared, confirming usability of guiacayl containing biopolymers as cathodes in Li-ion batteries. Lastly, naturally occurring polyphenol, tannic acid, was incorporated in fully bioderived hybrid material that shows performance comparable to commercial Li-ion batteries and good stability. This thesis presents an important advancement in understanding of biowaste derived cathode materials for Li-ion batteries. Further research should be conducted to better understand behaviour of guaiacyl groups during Li-ion battery cycling. Lastly, challenges of incorporation of lignin, an industrial biowaste, have to be addressed and lignin should be incorporated as a cathode material in Li-ion batteries.}, language = {en} } @phdthesis{Behrendt2018, author = {Behrendt, Felix Nicolas}, title = {New bio-based polymers}, url = {http://nbn-resolving.de/urn:nbn:de:kobv:517-opus4-418316}, school = {Universit{\"a}t Potsdam}, pages = {vii, 153}, year = {2018}, abstract = {Redox-responsive polymers, such as poly(disulfide)s, are a versatile class of polymers with potential applications including gene- and drug-carrier systems. Their degradability under reductive conditions allows for a controlled response to the different redox states that are present throughout the body. Poly(disulfide)s are typically synthesized by step growth polymerizations. Step growth polymerizations, however, may suffer from low conversions and therefore low molar masses, limiting potential applications. The purpose of this thesis was therefore to find and investigate new synthetic routes towards the synthesis of amino acid-based poly(disulfide)s. The different routes in this thesis include entropy-driven ring opening polymerizations of novel macrocyclic monomers, derived from cystine derivatives. These monomers were obtained with overall yields of up to 77\% and were analyzed by mass spectrometry as well as by 1D and 2D NMR spectroscopy. The kinetics of the entropy-driven ring-opening metathesis polymerization (ED-ROMP) were thoroughly investigated in dependence of temperature, monomer concentration, and catalyst concentration. The polymerization was optimized to yield poly(disulfide)s with weight average molar masses of up to 80 kDa and conversions of ~80\%, at the thermodynamic equilibrium. Additionally, an alternative metal free polymerization, namely the entropy-driven ring-opening disulfide metathesis polymerization (ED-RODiMP) was established for the polymerization of the macrocyclic monomers. The effect of different solvents, concentrations and catalyst loadings on the polymerization process and its kinetics were studied. Polymers with very high weight average molar masses of up to 177 kDa were obtained. Moreover, various post-polymerization reactions were successfully performed. This work provides the first example of the homopolymerization of endo-cyclic disulfides by ED-ROMP and the first substantial study into the kinetics of the ED-RODiMP process.}, language = {en} } @phdthesis{LorenteSanchez2017, author = {Lorente S{\´a}nchez, Alejandro Jose}, title = {Synthesis of side-chain polystyrenes for all organic solution processed OLEDs}, url = {http://nbn-resolving.de/urn:nbn:de:kobv:517-opus4-398006}, school = {Universit{\"a}t Potsdam}, pages = {xiv, 131}, year = {2017}, abstract = {In the present work side-chain polystyrenes were synthesized and characterized, in order to be applied in multilayer OLEDs fabricated by solution process techniques. Manufacture of optoelectronic devices by solution process techniques is meant to decrease significantly fabrication cost and allow large scale production of such devices. This dissertation focusses in three series, enveloped in two material classes. The two classes differ to each other in the type of charge transport exhibited, either ambipolar transport or electron transport. All materials were applied in all-organic solution processed green Ir-based devices. In the first part, a series of ambipolar host materials were developed to transport both charge types, holes and electrons, and be applied especially as matrix for green Ir-based emitters. It was possible to increase devices efficacy by modulating the predominant charge transport type. This was achieved by modification of molecules electron transport part with more electron-deficient heterocycles or by extending the delocalization of the LUMO. Efficiencies up to 28.9 cd/A were observed for all-organic solution-process three layer devices. In the second part, suitability of triarylboranes and tetraphenylsilanes as electron transport materials was studied. High triplet energies were obtained, up to 2.95 eV, by rational combination of both molecular structures. Although the combination of both elements had a low effect in materials electron transport properties, high efficiencies around 24 cd/A were obtained for the series in all-organic solution-processed two layer devices. In the last part, benzene and pyridine were chosen as the series electron-transport motif. By controlling the relative pyridine content (RPC) solubility into methanol was induced for polystyrenes with bulky side-chains. Materials with RPC ≥ 0.5 could be deposited orthogonally from solution without harming underlying layers. From the best of our knowledge, this is the first time such materials are applied in this architecture showing moderate efficiencies around 10 cd/A in all-organic solution processed OLEDs. Overall, the outcome of these studies will actively contribute to the current research on materials for all-solution processed OLEDs.}, language = {en} }