@article{ShashevKupschLangeetal.2017, author = {Shashev, Yury and Kupsch, Andreas and Lange, Axel and Evsevleev, Sergei and M{\"u}ller, Bernd R. and Osenberg, Markus and Manke, Ingo and Hentschel, Manfred P. and Bruno, Giovanni}, title = {Optimizing the visibility of X-ray phase grating interferometry}, series = {Materials testing : Materialpr{\"u}fung ; materials and components, technology and application}, volume = {59}, journal = {Materials testing : Materialpr{\"u}fung ; materials and components, technology and application}, publisher = {Hanser}, address = {M{\"u}nchen}, issn = {0025-5300}, doi = {10.3139/120.111097}, pages = {974 -- 980}, year = {2017}, abstract = {The performance of grating interferometers coming up now for imaging interfaces within materials depends on the efficiency (visibility) of their main component, namely the phase grating. Therefore, experiments with monochromatic synchrotron radiation and corresponding simulations are carried out. The visibility of a phase grating is optimized by different photon energies, varying detector to grating distances and continuous rotation of the phase grating about the grid lines. Such kind of rotation changes the projected grating shapes, and thereby the distribution profiles of phase shifts. This yields higher visibilities than derived from ideal rectangular shapes. By continuous grating rotation and variation of the propagation distance, we achieve 2D visibility maps. Such maps provide the visibility for a certain combination of grating orientation and detector position. Optimum visibilities occur at considerably smaller distances than in the standard setup.}, language = {en} } @article{SunOsenbergDongetal.2018, author = {Sun, Fu and Osenberg, Markus and Dong, Kang and Zhou, Dong and Hilger, Andre and Jafta, Charl J. and Risse, Sebastian and Lu, Yan and Markoetter, Henning and Manke, Ingo}, title = {Correlating Morphological Evolution of Li Electrodes with Degrading Electrochemical Performance of Li/LiCoO2 and Li/S Battery Systems}, series = {ACS energy letters / American Chemical Society}, volume = {3}, journal = {ACS energy letters / American Chemical Society}, number = {2}, publisher = {American Chemical Society}, address = {Washington}, issn = {2380-8195}, doi = {10.1021/acsenergylett.7b01254}, pages = {356 -- 365}, year = {2018}, abstract = {Efficient Li utilization is generally considered to be a prerequisite for developing next-generation energy storage systems (ESSs). However, uncontrolled growth of Li microstructures (LmSs) during electrochemical cycling has prevented its practical commercialization. Herein, we attempt to understand the correlation of morphological evolution of Li electrodes with degrading electrochemical performances of Li/LiCoO2 and Li/S systems by synchrotron X-ray phase contrast tomography technique. It was found that the continuous transformation of the initial dense Li bulk to a porous lithium interface (PL1) structure intimately correlates with the gradually degrading overall cell performance of these two systems. Additionally, the formation mechanism of the PLI and its correlation with previously reported inwardly growing LmS and the lithium-reacted region have been intensively discussed. The information that we gain herein is complementary to previous investigations and may provide general insights into understanding of degradation mechanisms of Li metal anodes and also provide highly needed guidelines for effective design of reliable next-generation Li metal-based ESSs.}, language = {en} } @article{SunDongOsenbergetal.2018, author = {Sun, Fu and Dong, Kang and Osenberg, Markus and Hilger, Andre and Risse, Sebastian and Lu, Yan and Kamm, Paul H. and Klaus, Manuela and Markoetter, Henning and Garcia-Moreno, Francisco and Arlt, Tobias and Manke, Ingo}, title = {Visualizing the morphological and compositional evolution of the interface of InLi-anode|thio-LISION electrolyte in an all-solid-state Li-S cell by in operando synchrotron X-ray tomography and energy dispersive diffraction}, series = {Journal of materials chemistry : A, Materials for energy and sustainability}, volume = {6}, journal = {Journal of materials chemistry : A, Materials for energy and sustainability}, number = {45}, publisher = {Royal Society of Chemistry}, address = {Cambridge}, issn = {2050-7488}, doi = {10.1039/c8ta08821g}, pages = {22489 -- 22496}, year = {2018}, abstract = {Dynamic and direct visualization of interfacial evolution is helpful in gaining fundamental knowledge of all-solid-state-lithium battery working/degradation mechanisms and clarifying future research directions for constructing next-generation batteries. Herein, in situ and in operando synchrotron X-ray tomography and energy dispersive diffraction were simultaneously employed to record the morphological and compositional evolution of the interface of InLi-anode|sulfide-solid-electrolyte during battery cycling. Compelling morphological evidence of interfacial degradation during all-solid-state-lithium battery operation has been directly visualized by tomographic measurement. The accompanying energy dispersive diffraction results agree well with the observed morphological deterioration and the recorded electrochemical performance. It is concluded from the current investigation that a fundamental understanding of the phenomena occurring at the solid-solid electrode|electrolyte interface during all-solid-state-lithium battery cycling is critical for future progress in cell performance improvement and may determine its final commercial viability.}, language = {en} }